Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Gravity = 1.53 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D792
Solvay Specialty Polymers AvaSpire® AV-848 GF30 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-848 GF30 is a 30% glass fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable gra..
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D792
PolyOne Geon™ Vinyl Flexible R158AE Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Specific Gravity 1.53 g/cc
1.53 g/cc
ISO 1183
Lehmann & Voss LUVOCOM® 1850-7431 PBT, with carbon fiber and glass spheres
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Low warpage.Low waterabsorbtion, for dimensional stable precision parts.Par..
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D792
LG Chemical LUPOY GP-2401F General Purpose Modified PC, 40% Glass Fiber Reinforced, Flame Retardant
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
Specific Gravity 1.53 g/cc

@Temperature 25.0 °C
1.53 g/cc

@Temperature 77.0 °F
STM 2
Lord Adhesives Thermosetâ„¢ EP-809 Ignition Coil Impregnating and Encapsulation Epoxy
Lord EP-809 is a long working life, heat curing, two component epoxy formulation. It was designed especially for potting high voltage automotive ignition coils. The combination of low viscosity, exc..
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D792
Gromax PBT 4115-104D 15% Glass Fiber Filled
Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
Specific Gravity 1.53 g/cc
1.53 g/cc
Kuraray Genestarâ„¢ GP2450NH-2 Nylon, 45% Glass Filled
Standard V-0 Grade. Halogen free, following the standards that Br is less than 900ppm, Cl is less than 900ppm, and total of halogen amount (Br and Cl) is less than 1500ppm.This grade meets UL94, V-0..
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D 792
MRC Polymers MAXNITEâ„¢ 550 GF30 PET, 30% Glass Mineral Reinforced
Information provided by MRC Polymers Inc.
Specific Gravity 1.53 g/cc
1.53 g/cc
ISO 1183
Lehmann & Voss LUVOCOM® 1105-7860/GY7037 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High dimensionally stable precision parts, high continuous use tempera..
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D792
SABIC Innovative Plastics ULTEM SF2360 PEI Blend (Asia Pacific)
High flow Ultem for thin wall application
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D792
SABIC Innovative Plastics Valox® 420 PBT (Europe-Africa-Middle East)
VALOX 420 is a 30% glass fiber reinforced PBT injection moulding resin with excellent mechanical and thermal properties. Applications: appliance handles, spotlights, electric motors.
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D 792
SABIC Innovative Plastics Valox® 420M PBT (Asia Pacific)
30% GR PBTP. Easy flow/release. High stiffness and load bearing properties.This data was supplied by SABIC-IP for the Asia Pacific region.
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D792
SABIC Innovative Plastics Valox® IQNH4550 PBT
Valox* iQNH4550 resin is a glass filled, non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 31% ..
Specific Gravity 1.53 g/cc
1.53 g/cc
Silberline SparkleBriteâ„¢ 190NL-DL
SparkleBriteâ„¢ "DL" pigments are non-leafing aluminum pigment pastes carried in a glycol. These grades are based on cornflake geometry and produce strong metallic effects in flexographic and gra..
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D792
A. Schulman POLYBATCH™ White 8350/UV5 Concentrate Based In Polyethylene
DescriptionPOLYBATCH® 8350/UV5 is a specialty white color concentrate containing an optimized blend of white and UV stabilizer based in polyethylene. POLYBATCH® 8350/UV5 has been designed to prov..
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D792
A. Schulman SCHULADUR® A GF30 30% Glass Fiber Reinforced PBT
Information provided by A. Schulman.
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D792
A. Schulman SCHULADUR® A GF30 30% Glass Fiber Reinforced PBT
Information provided by A. Schulman.
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D792
A. Schulman SCHULADUR® A GF30 30% Glass Fiber Reinforced PBT
Information provided by A. Schulman.
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D792
A. Schulman POLYBATCH™ White 8350/UV5 Concentrate Based In Polyethylene
DescriptionPOLYBATCH® 8350/UV5 is a specialty white color concentrate containing an optimized blend of white and UV stabilizer based in polyethylene. POLYBATCH® 8350/UV5 has been designed to prov..
Copyright © lookpolymers.com All Rights Reserved