Material Notes:
Dry as molded.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D955
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 85.5 MPa
12400 psi
ASTM D638
Elongation at Break 10 %
10 %
ASTM D638
Flexural Modulus 3.00 GPa
435 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 216 °C
421 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 74.0 °C
165 °F
ASTM D648