Material Notes:
Information provided by Niche Polymer
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0500 cm/cm
0.0500 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 138 MPa
20000 psi
ASTM D638
Elongation at Break 2.50 %
2.50 %
ASTM D638
Flexural Strength 193 MPa
28000 psi
ASTM D790
Flexural Modulus 7.58 GPa
1100 ksi
ASTM D790
Izod Impact, Unnotched 0.427 J/cm

@Thickness 3.17 mm
0.800 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 245 °C
473 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 254 - 271 °C
489 - 520 °F
ASTM D789
Descriptive Properties Value Comments
Color Black
Copyright © lookpolymers.com All Rights Reserved