NOVA Chemicals Sclair® 97B HDPE Blow Molding Resin  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Extruded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Sclair® 97B HDPE Blow Molding Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Good impact strength, easy processability, high ESCR.Applications: Small part blow molding, high ESCR HIC applications.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ASTM D792
Environmental Stress Crack Resistance 200 hour
200 hour
F50, Condition A, ASTM D1693
Melt Flow 0.67 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.67 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 64.6
64.6
ASTM D2240
Tensile Strength, Yield 23.0 MPa
3340 psi
ASTM D638
Elongation at Break 1000 %
1000 %
ASTM D638
Flexural Modulus 0.758 GPa
110 ksi
ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 123 °C
253 °F
ASTM D1525
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
ASTM D696
Processing Properties Metric English Comments
Melt Temperature 160 - 205 °C
320 - 401 °F