NatureWorks® Ingeo™ 7032D Stretch Blow Molding/Bottle Grade PLA

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polylactic Acid (PLA) Biopolymer
Manufacturer NatureWorks LLC
Trade Name Ingeo™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NatureWorks® Ingeo™ 7032D Stretch Blow Molding/Bottle Grade PLA.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
NatureWorks® PLA polymer 7032D is a bottles grade resin designed for injection stretch blow molded applications where heat setting is needed. PLA polymer 7032D can be run on conventional ISBM equipment. 7032D is typically run at lower processing temperatures than bottle grade PET.Applications: Injection Stretch Blow Molded Bottles for 1:2 stage operations. Ideal for applications where heat setting is required such as Fruit juices, Sports drinks, Jams and Jellies
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D792
Melt Density 1.08 - 1.12 g/cc

@Temperature 230 °C
0.0390 - 0.0405 lb/in³

@Temperature 446 °F
ASTM D1238
Linear Mold Shrinkage 0.003 - 0.005 cm/cm
0.003 - 0.005 in/in
Melt Flow 5.0 - 15 g/10 min

@Load 2.16 kg,
Temperature 210 °C
5.0 - 15 g/10 min

@Load 4.76 lb,
Temperature 410 °F
ASTM D1238
Thermal Properties Metric English Comments
Melting Point 160 °C
320 °F
ASTM D3418
Glass Transition Temp, Tg 55.0 - 60.0 °C
131 - 140 °F
ASTM D3417
Processing Properties Metric English Comments
Feed Temperature 180 °C
356 °F
Nozzle Temperature 210 - 220 °C
410 - 428 °F
Melt Temperature 200 - 220 °C
392 - 428 °F
Mold Temperature 21.0 - 38.0 °C
69.8 - 100 °F
Back Pressure 0.689 - 1.38 MPa
100 - 200 psi