Physical Properties Metric English Comments
Melt Density 1.08 g/cc

@Temperature 230 °C
0.0390 lb/in³

@Temperature 446 °F
ASTM D1238
NatureWorks® Ingeo™ 6060D Fiber Grade PLA
NatureWorks PLA polymer 6060D is an amorphous thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6060D is designed for extrusion into mech..
Melt Density 1.08 g/cc

@Temperature 230 °C
0.0390 lb/in³

@Temperature 446 °F
ASTM D1238
NatureWorks® Ingeo™ 6201D Fiber Grade PLA
NatureWorks® PLA polymer 6201D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6201D is designed for extrusion into mechanically ..
Melt Density 1.08 g/cc

@Temperature 230 °C
0.0390 lb/in³

@Temperature 446 °F
ASTM D1238
NatureWorks® Ingeo™ 6202D Fiber Grade PLA
NatureWorks® PLA polymer 6202D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6202D is designed for extrusion into mechanically ..
Melt Density 1.08 g/cc

@Temperature 230 °C
0.0390 lb/in³

@Temperature 446 °F
ASTM D1238
NatureWorks® Ingeo™ 6204D Fiber Grade PLA
NatureWorks® PLA polymer 6204D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6204D is designed for extrusion into mechanically ..
Melt Density 1.08 g/cc

@Temperature 230 °C
0.0390 lb/in³

@Temperature 446 °F
ASTM D1238
NatureWorks® Ingeo™ 6251D Fiber Grade PLA
NatureWorks® PLA polymer 6251D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6251D is designed for spunbond products using conv..
Melt Density 1.08 g/cc

@Temperature 230 °C
0.0390 lb/in³

@Temperature 446 °F
ASTM D1238
NatureWorks® Ingeo™ 6302D Fiber Grade PLA
NatureWorks PLA polymer 6302D is an amorphous thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6302D is designed for extrusion into mech..
Melt Density 1.08 g/cc

@Temperature 230 °C
0.0390 lb/in³

@Temperature 446 °F
ASTM D1238
NatureWorks® Ingeo™ 6751D Fiber Grade PLA
NatureWorks® PLA polymer 6751D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6751D is designed for extrusion into mechanically ..
Melt Density 1.08 - 1.12 g/cc

@Temperature 230 °C
0.0390 - 0.0405 lb/in³

@Temperature 446 °F
ASTM D1238
NatureWorks® Ingeo™ 7032D Stretch Blow Molding/Bottle Grade PLA
NatureWorks® PLA polymer 7032D is a bottles grade resin designed for injection stretch blow molded applications where heat setting is needed. PLA polymer 7032D can be run on conventional ISBM equip..
Melt Density 1.08 g/cc

@Temperature 285 °C
0.0390 lb/in³

@Temperature 545 °F
ASTM D1238
Eastman Eastar 5445 PCTG Copolyester, Injection Molded  (discontinued **)
Eastar PCTG 5445 is an amorphous copolyester. Because of its clarity, toughness and good melt strength, Eastar PCTG Copolyester 5445 is useful in a number of applications. It has high gloss and is t..
Melt Density 1.08 g/cc

@Temperature 285 °C
0.0390 lb/in³

@Temperature 545 °F
ASTM D1238
Eastman Eastar 5445 PCTG Copolyester, Film  (discontinued **)
Eastar PCTG 5445 is an amorphous copolyester. Because of its clarity, toughness and good melt strength, Eastar PCTG Copolyester 5445 is useful in a number of applications. It has high gloss and is t..
Melt Density 1.08 g/cc

@Temperature 230 °C
0.0390 lb/in³

@Temperature 446 °F
ASTM D1238
NatureWorks® Ingeo™ 6252D Meltblown Fiber Grade Biopolymer
NatureWorks® PLA polymer 6252D is a thermoplastic fiber-grade resin derived from annually renewable resources. Available in lubricated pellet form, 6252D is designed for meltblown products using co..
Melt Density 1.08 g/cc

@Temperature 230 °C
0.0390 lb/in³

@Temperature 446 °F
ASTM D1238
NatureWorks® Ingeo™ 6350D Fiber Grade PLA
NatureWorks PLA polymer 6350D is an amorphous thermoplastic spunbond-grade resin derived primarily from annually renewable resources. Available in pellet form, 6350D is designed for extrusion into s..
Melt Density 1.08 g/cc

@Temperature 230 °C
0.0390 lb/in³

@Temperature 446 °F
ASTM D1238
NatureWorks® Ingeo™ 6400D Fiber Grade PLA
NatureWorks® PLA polymer 6400D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6400D is designed for extrusion into mechanically ..
Melt Density 1.08 g/cc

@Temperature 230 °C
0.0390 lb/in³

@Temperature 446 °F
ASTM D1238
NatureWorks® Ingeo™ 6752D Spunbond Grade Biopolymer
Sheath polymer for spunbound uses. NatureWorks® PLA polymer 6752D, a NatureWorks LLC product, is a thermoplastic fiber-grade resin de-rived from annually renewable resources. Available in pellet f..
Melt Density 1.08 g/cc
0.0390 lb/in³
Styron MAGNUMâ„¢ 357 HP Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: MAGNUMâ„¢ ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositi..
Melt Density 1.08 g/cc
0.0390 lb/in³
Melt density
Styron Magnumâ„¢ 344HP ABS
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Melt Density 1.08 g/cc
0.0390 lb/in³
Melt density
Styron Magnumâ„¢ 357HP ABS, High Heat
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..