Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 55.0 - 60.0 °C | 131 - 140 °F | ASTM D3418 |
NatureWorks® Ingeo™ 3052D Lubricated, High Flow Biopolymer NatureWorks® PLA polymer 2003D is a thermoplastic resin derived from annually renewable resources. It is designed for injection molding applications where the requirements are clarity with heat def.. |
|||
Glass Transition Temp, Tg | 55.0 - 60.0 °C | 131 - 140 °F | ASTM D3417 |
NatureWorks® Ingeo™ 6201D Fiber Grade PLA NatureWorks® PLA polymer 6201D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6201D is designed for extrusion into mechanically .. |
|||
Glass Transition Temp, Tg | 55.0 - 60.0 °C | 131 - 140 °F | ASTM D3417 |
NatureWorks® Ingeo™ 6202D Fiber Grade PLA NatureWorks® PLA polymer 6202D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6202D is designed for extrusion into mechanically .. |
|||
Glass Transition Temp, Tg | 55.0 - 60.0 °C | 131 - 140 °F | ASTM D3417 |
NatureWorks® Ingeo™ 7032D Stretch Blow Molding/Bottle Grade PLA NatureWorks® PLA polymer 7032D is a bottles grade resin designed for injection stretch blow molded applications where heat setting is needed. PLA polymer 7032D can be run on conventional ISBM equip.. |
|||
Glass Transition Temp, Tg | 55.0 - 60.0 °C | 131 - 140 °F | ASTM D3418 |
NatureWorks® Ingeo™ 8052D Foam Grade Biopolymer Ingeo 8052D can be converted into an expanded foam sheet with use temperatures up to 77°F (25°C). This foam is lightweight, strong and suitable for packaging fresh meat and vegetables. In order to.. |
|||
Glass Transition Temp, Tg | 55.0 °C | 131 °F | DSC, both heating and cooling speeds of 20°C/min |
Noltex Soarnol® A4412 Ethylene Vinyl Alcohol Copolymer Ethylene content 44 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows design of lower cost packages by using a.. |
|||
Glass Transition Temp, Tg | 55.0 °C | 131 °F | 10°C/min; ISO 11357-1/-2 |
DuPont Performance Polymers Crastin® S600F40 NC010 PBT
(Unverified Data**) Crastin® S600F40 NC010 is an unreinforced, lubricated, low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Glass Transition Temp, Tg | 55.0 - 60.0 °C | 131 - 140 °F | ASTM D3417 |
NatureWorks® Ingeo™ 6350D Fiber Grade PLA NatureWorks PLA polymer 6350D is an amorphous thermoplastic spunbond-grade resin derived primarily from annually renewable resources. Available in pellet form, 6350D is designed for extrusion into s.. |
|||
Glass Transition Temp, Tg | 55.0 - 60.0 °C | 131 - 140 °F | ASTM D3417 |
NatureWorks® Ingeo™ 6400D Fiber Grade PLA NatureWorks® PLA polymer 6400D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6400D is designed for extrusion into mechanically .. |
|||
Glass Transition Temp, Tg | 55.0 - 60.0 °C | 131 - 140 °F | ASTM D3417 |
NatureWorks® Ingeo™ 6752D Spunbond Grade Biopolymer Sheath polymer for spunbound uses. NatureWorks® PLA polymer 6752D, a NatureWorks LLC product, is a thermoplastic fiber-grade resin de-rived from annually renewable resources. Available in pellet f.. |
|||
Glass Transition Temp, Tg | 55.0 °C | 131 °F | Dynamic Viscoelasticity |
EVALCA EVAL® LC-E105A Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 44 mol % Ethylene.Data provided by EVALCA. Applications: Cast film, melt phase forming, solid phase pressure forming, tubes, coex coating. EVOH is used in packaging applications because of its out.. |
|||
Glass Transition Temp, Tg | 55.0 °C | 131 °F | |
Styron DL 295 Carboxylated SB Performance Features: General purpose wood adhesiveApplications: General Purpose Adhesive and Wood Adhesive (EPI)EuropeInformation provided by Styron |
|||
Glass Transition Temp, Tg | 55.0 °C | 131 °F | Ultimate Tg |
Tra-Con Tra-Bond 2115 Clear High Strength Epoxy Adhesive TRA-BOND 2115 is a clear, low viscosity epoxy formulation used in the fabrication of lasers. It is capable of withstanding 30 seconds of 60 watt direct laser energy. The low cure shrinkage (using a .. |
|||
Glass Transition Temp, Tg | 55.0 °C | 131 °F | ETM 300-90 |
ExxonMobil ESCOREZ™ 5300 Petroleum Hydrocarbon Resin The Escorez 5300 series resins are water white cycloaliphatic hydrocarbon resins. They are designed to tackify a variety of adhesive polymers including EVA, SIS and SEBS block copolymers, APP an d A.. |
|||
Glass Transition Temp, Tg | 55.0 °C | 131 °F | 10°C/min; ISO 11357-1/-2 |
DuPont Performance Polymers Crastin® FGS600F10 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Polybutylene Terephthalate Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Glass Transition Temp, Tg | 55.0 °C | 131 °F | 10°C/min; ISO 11357-1/-2 |
DuPont Performance Polymers Crastin® S600F40 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced Low Viscosity Polybutylene Terephthalate Crastin S600F40 NC010 is an unreinforced lubricated low viscosity polybutylene terephthalate resin for injection molding.Information provided by.. |
|||
Glass Transition Temp, Tg | >= 55.0 °C | >= 131 °F | Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min |
Epoxy Technology EPO-TEK® 302-3M Optically Transparent Epoxy Product Description: EPO-TEK® 302-3M is a two component epoxy used for optical, medical, fiber optic, and semiconductor applications. The epoxy is good for adhesive joining, sealing, potting, or as.. |
|||
Glass Transition Temp, Tg | >= 55.0 °C | >= 131 °F | Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min |
Epoxy Technology EPO-TEK® 320 Optical, Opaque Epoxy Product Description: EPO-TEK® 320 is a two component, black-colored and optically opaque epoxy designed for optical, medical, and optoelectronic packaging of semiconductor devices and components. .. |
|||
Glass Transition Temp, Tg | >= 55.0 °C | >= 131 °F | Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min |
Epoxy Technology EPO-TEK® 320-LV Optically Opaque Epoxy Material Description: A two component, optically opaque epoxy adhesive designed for semiconductor and PCB applications in optoelectronic instrumentation and assemblies. A lower viscosity version of.. |
|||
Glass Transition Temp, Tg | >= 55.0 °C | >= 131 °F | Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min |
Epoxy Technology EPO-TEK® 731 Epoxy Adhesive Material Description: A two component, thixotropic, room temperature-curing epoxy adhesive. It is an electrically and thermally insulating epoxy designed for general applications in semiconductor p.. |
|||
Glass Transition Temp, Tg | >= 55.0 °C | >= 131 °F | Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min |
Epoxy Technology EPO-TEK® OE121 Black Epoxy Adhesive Material Description: A two component, low temperature curing epoxy adhesive designed for semiconductor flip chip underfill. It is color coded black for visual ID during the underfilling process. .. |
|||
Glass Transition Temp, Tg | 55.0 °C | 131 °F | |
Armstrong A-7 Epoxy Adhesive Clear, flexible, 5-minute cure structural bonding plastic adhesive. Develops high performance, high impact durable bonds for operating temperatures from -65° to +250°. Supplied in 1:1 ratio dispe.. |
|||
Glass Transition Temp, Tg | 55.0 - 132 °C | 131 - 270 °F | Average value: 92.8 °C Grade Count:6 |
Overview of materials for Epoxy, Cast, Metal Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Aluminum Filled". Each property range of values reported is minimum and maximum values of a.. |
|||
Glass Transition Temp, Tg | 55.0 °C | 131 °F | TM R050-25 |
Resinlab® EP1115 Clear Unfilled Epoxy Adhesive Resinlab™ EP1115 Clear is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. This product gives good resistance to water, salt spray, inorganic acids and.. |
|||
Glass Transition Temp, Tg | 55.0 °C | 131 °F | |
Loctite® Durabond® E-60NC Epoxy Adhesive Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli.. |