Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Mold Temperature = 69.8 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Mold Temperature 21.0 - 38.0 °C
69.8 - 100 °F
NatureWorks® Ingeo™ 7032D Stretch Blow Molding/Bottle Grade PLA
NatureWorks® PLA polymer 7032D is a bottles grade resin designed for injection stretch blow molded applications where heat setting is needed. PLA polymer 7032D can be run on conventional ISBM equip..
Mold Temperature 21.0 - 49.0 °C
69.8 - 120 °F
Advanced Elastomer Systems VistaFlex® 641N Thermoplastic Rubber  (discontinued **)
A translucent thermoplastic elastomer with snappiness. It can be processed using injection molding or extrusion processing techniques.Key Features: Flex modulus (1% Secant) 7.2 MPa (1050 psi); Vica..
Mold Temperature 21.0 - 49.0 °C
69.8 - 120 °F
Advanced Elastomer Systems Vistaflex® 671N Thermoplastic Rubber  (discontinued **)
A translucent thermoplastic elastomer with snappiness. It can be processed using injection molding or extrusion processing techniques.Key Features: Flex modulus (1% Secant) 9.0 MPa (1300 psi); Vica..
Mold Temperature 21.0 - 49.0 °C
69.8 - 120 °F
Elastocon TPE Technologies Elastocon® SMR1000 Thermoplastic Polyolefin Elastomer
Elastocon® SMR1000 thermoplastic polyolefin elastomer has been developed for applications that require impact resistance and a high gloss scratch and mar resistant surface finish. Elastocon® SMR10..
Mold Temperature 21.0 - 49.0 °C
69.8 - 120 °F
Elastocon TPE Technologies Elastocon® SMR1450 Thermoplastic Polyolefin Elastomer
Elastocon® SMR1450 thermoplastic polyolefin elastomer has been developed for applications that require low temperature impact resistance and a high gloss scratch and mar resistant surface finish. E..
Mold Temperature 21.0 - 49.0 °C
69.8 - 120 °F
Elastocon TPE Technologies Elastocon® SMR1555 Thermoplastic Polyolefin Elastomer
Elastocon® SMR1555 thermoplastic polyolefin elastomer has been developed for applications that require low temperature impact resistance and a high gloss scratch and mar resistant surface finish. E..
Mold Temperature 21.0 - 49.0 °C
69.8 - 120 °F
Elastocon TPE Technologies Elastocon® SMR1600 Thermoplastic Polyolefin Elastomer
Elastocon® SMR1600 thermoplastic polyolefin elastomer has been developed for applications that require low temperature impact resistance and a high gloss scratch and mar resistant surface finish. E..