Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 1.20 g/cc | 0.0434 lb/in³ | Tapped |
Nyco M325 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Bulk Density | 1.20 g/cc | 0.0434 lb/in³ | Tapped |
Nyco NYAD® 325 Wollastonite Powdered grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particl.. |
|||
Bulk Density | 1.20 g/cc | 0.0434 lb/in³ | Loose |
Nyco NYGLOS® M50 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Bulk Density | 1.20 g/cc | 0.0434 lb/in³ | Tapped |
Nyco NYGLOS® STPO Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Bulk Density | 1.20 - 1.30 g/cc | 0.0434 - 0.0470 lb/in³ | |
Nabaltec GRANALOX® NM 9212 F Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Bulk Density | 1.20 - 1.35 g/cc | 0.0434 - 0.0488 lb/in³ | |
Nabaltec GRANALOX® NM 9510 F Ceramic Body Nabaltec's GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Bulk Density | 1.20 - 1.35 g/cc | 0.0434 - 0.0488 lb/in³ | |
Nabaltec GRANALOX® NM 9634 F Ceramic Body Nabaltec's GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Bulk Density | 1.20 g/cc | 0.0434 lb/in³ | ASTM D4894 |
3M Dyneon™ CC646/S Custom Compound
(discontinued **) This compound consists of a mixture of 60% bronze blended with PTFE.Information provided by Dyneon, A 3M Company |
|||
Bulk Density | 1.20 - 1.30 g/cc | 0.0434 - 0.0470 lb/in³ | After drying at 110°C |
Gouda Vuurvast GOLITE 110 Refractory Insulating Castable Description: Golite 110 is composed of a light weight refractory aggregate plus several additives to improve the mechanical and refractory properties.Remarks: These values apply to cast products. Al.. |
|||
Bulk Density | 1.20 g/cc | 0.0434 lb/in³ | of Dry Beads |
Mo-Sci Corporation GL-0179 Borosilicate Glass Spheres Appearance: Solid clear borosilicate glass microspheres with white color in powder form.Typical applications of GL0179 beads include: calibration, high temperature spacer material for gauge control,.. |
|||
Bulk Density | 1.20 g/cc | 0.0434 lb/in³ | of Dry Beads |
Mo-Sci Corporation GL-0186 Borosilicate Glass Spheres Appearance: Solid clear borosilicate glass microspheres with white color in powder form.Typical applications of GL0186 beads include: high temperature spacer material for gauge control, coating, fil.. |
|||
Bulk Density | 1.20 g/cc | 0.0434 lb/in³ | of Dry Beads |
Mo-Sci Corporation GL-0263 Cu Coated Borosilicate Glass Spheres Appearance: Solid borosilicate glass microspheres with metallic copper coatingTypical applications of GL-0263 glass microspheres include: conductive filler for plastic, pigment, and etc.Information .. |
|||
Bulk Density | <= 1.20 g/cc | <= 0.0434 lb/in³ | Dried at 110°C |
Sharadaa Ceramics REFINSUL ZAP-018 Insulating Castables Description: We provide our clients a range of Insulating Castables, that are used as backup layer in process industries and hot face layer in petrochemical industry. These castables are known for l.. |
|||
Bulk Density | 1.20 g/cc @Temperature 200 °C |
0.0434 lb/in³ @Temperature 392 °F |
|
Sharadaa Ceramics Sharada LTM 1.2 Insulating Castable Low Density/ High Strength Insulating Castable-Low Thermal Mass LiningInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Bulk Density | 1.20 g/cc | 0.0434 lb/in³ | Dry |
Skamol Group VIP 12 Vermiculite Insulating Slab SKAMOL V-1100 & VIP-12 vermiculite slabs have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulation of all refractory constr.. |
|||
Bulk Density | 1.20 g/cc | 0.0434 lb/in³ | Loose |
Excalibar ExBar™ W 4 Barite BaSO4 Powder ExBar™ W high-purity white barytes are manufactured using only the highest quality white, natural barium sulfate ore. Strict quality control results in consistent products that are used in paints, .. |
|||
Bulk Density | 1.20 g/cc | 0.0434 lb/in³ | |
Daikin NEOFLON AP-201SH PFA Semiconductor Grade NEOFLON PFA semiconductor grade.Applications: Good fluidity, suited to making moldings of complex shapes, requiring high fluidity.Information provided by Daikin Industries. |
|||
Bulk Density | 1.20 g/cc | 0.0434 lb/in³ | |
Daikin NEOFLON AP-211SH PFA Semiconductor Grade NEOFLON PFA semiconductor grade.Applications: Tubing and injection molded parts requiring high stress crack resistance, etc.Information provided by Daikin Industries. |
|||
Bulk Density | 1.20 g/cc | 0.0434 lb/in³ | |
Daikin NEOFLON AP-221SH PFA Semiconductor Grade NEOFLON PFA semiconductor grade.Applications: Linings, tubing, etc.Information provided by Daikin Industries. |
|||
Bulk Density | 1.20 g/cc | 0.0434 lb/in³ | |
Daikin NEOFLON AP-230ASL PFA Pellets NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Anti-static grader for extrusion molded parts. Piping, tube, etc... |
|||
Bulk Density | 1.20 g/cc | 0.0434 lb/in³ | |
Daikin NEOFLON NP-101 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: High speed wire and cable coatings.Information pro.. |
|||
Bulk Density | 1.20 g/cc | 0.0434 lb/in³ | |
Daikin NEOFLON NP-21 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, injection molding.Applications: Suited to high speed extrusion .. |
|||
Bulk Density | 1.20 g/cc | 0.0434 lb/in³ | |
Daikin NEOFLON NP-40 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, transfer molding, compression molding.Applications: Films and s.. |
|||
Bulk Density | >= 1.20 g/cc | >= 0.0434 lb/in³ | |
Chosun Refractories C-2 Insulating Firebrick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 1.20 g/cc | 0.0434 lb/in³ | |
Chosun Refractories LWB-120 Casting Block Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 1.20 g/cc | 0.0434 lb/in³ | Tapped |
CIMBAR EliteTalc® 20 Cosmetic Talc Cimbar performance Minerals MV, LLC Talc U.S.P. Cosmetic talcs are designed specifically for cosmetic formulations. Talc is commonly used in cosmetics for its ability to bind to oils, create a mois.. |
|||
Bulk Density | 1.20 g/cc | 0.0434 lb/in³ | |
Daikin NEOFLON AP-201 PFA Pellets NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Complicated injection molded parts requiring high melt flow to fil.. |
|||
Bulk Density | 1.20 g/cc | 0.0434 lb/in³ | |
Daikin NEOFLON AP-230 PFA Pellets NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Linings, tubing, etc.Information provided by Daikin Industries. |
|||
Bulk Density | 1.20 g/cc | 0.0434 lb/in³ | |
Daikin NEOFLON AP-231SH PFA Semiconductor Grade NEOFLON PFA semiconductor grade.Applications: Linings, tubing, etc.Information provided by Daikin Industries. |
|||
Bulk Density | 1.20 g/cc | 0.0434 lb/in³ | |
Daikin NEOFLON NP-20 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, injection molding.Applications: Wire and cable coatings, films,.. |