Processing Properties | Metric | English | Comments |
---|---|---|---|
Sintering Temperature | 1550 - 1650 °C | 2820 - 3000 °F | Interval (dense ceramic parts) |
Nabaltec GRANALOX® NM 9212 E Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Sintering Temperature | 1550 - 1650 °C | 2820 - 3000 °F | Interval (dense ceramic parts) |
Nabaltec GRANALOX® NM 9212 F Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Sintering Temperature | 1500 - 1650 °C | 2730 - 3000 °F | Interval (dense ceramic parts) |
Nabaltec GRANALOX® NM 9216 Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Sintering Temperature | 1550 - 1650 °C | 2820 - 3000 °F | Interval (dense ceramic parts) |
Nabaltec GRANALOX® NM 9510 F Ceramic Body Nabaltec's GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |