Material Notes:
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum are tailored to the application areas in which the material is used such as wear resistance, high temperature stability, good electrical insulation, thermal conductivity and corrosion resistance.Used in machinery parts and ballistic ceramics.
Physical Properties Metric English Comments
Bulk Density 1.25 - 1.35 g/cc
0.0452 - 0.0488 lb/in³
Density 3.60 - 3.65 g/cc
0.130 - 0.132 lb/in³
Sintered Density
Moisture Absorption at Equilibrium 0.20 - 0.50 %
0.20 - 0.50 %
Loss On Ignition 5.5 %
5.5 %
Particle Size 180 - 230 µm
180 - 230 µm
Median Grain Diameter
Thermal Properties Metric English Comments
Shrinkage 15 - 16 %
15 - 16 %
linear
Component Elements Properties Metric English Comments
Al2O3 92 %
92 %
Na2O 0.30 %
0.30 %
Processing Properties Metric English Comments
Sintering Temperature 1550 °C
2820 °F
1500 - 1650 °C
2730 - 3000 °F
Interval (dense ceramic parts)
Descriptive Properties Value Comments
Dwell Time hr. 1
Copyright © lookpolymers.com All Rights Reserved