Asahi Kasei Thermylene® P-9900-0712 Chemically Coupled Polypropylene Compound

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Asahi Kasei
Trade Name Thermylene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Kasei Thermylene® P-9900-0712 Chemically Coupled Polypropylene Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Automotive: Blower Wheels, HVAC Electrical and Specialty: Flush Valves, Pump BasesInformation provided by Asahi Kasei
Physical Properties Metric English Comments
Melt Flow 17 g/10 min
17 g/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Yield 34.5 MPa
5000 psi
Elongation at Yield 35 %
35 %
Flexural Modulus 1.72 GPa
250 ksi
Izod Impact, Notched 0.481 J/cm
0.900 ft-lb/in
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 93.0 °C
199 °F
Flammability, UL94 HB
HB