Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 180 - 230 µm | 180 - 230 µm | Median Granulate Size |
Nabaltec GRANALOX® NM 9212 E Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Particle Size | 180 - 230 µm | 180 - 230 µm | Median Grain Diameter |
Nabaltec GRANALOX® NM 9216 Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Particle Size | 180 - 230 µm | 180 - 230 µm | Median Grain Diameter |
Nabaltec GRANALOX® NM 9612 Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Particle Size | 180 - 230 µm | 180 - 230 µm | Median Grain Diameter |
Nabaltec GRANALOX® NM 9620 Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Particle Size | 180 - 230 µm | 180 - 230 µm | Median Grain Diameter |
Nabaltec GRANALOX® NM 9622 Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Particle Size | 180 - 230 µm | 180 - 230 µm | Median Grain Diameter |
Nabaltec GRANALOX® NM 9816 Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Particle Size | 180 - 220 µm | 180 - 220 µm | Mean Granulate Size |
Nabaltec GRANALOX® NM 9922 B Ceramic Body, Binder Free Nabaltec offers ceramic bodies with different alumina content as free-of-binder grades. With the addition of necessary amount of water (approx. 20 %) these grades can be directly used for slip casti.. |
|||
Particle Size | 180 - 230 µm | 180 - 230 µm | Median Grain Diameter |
Nabaltec GRANALOX® NM 9923 Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Particle Size | 180 - 250 µm | 180 - 250 µm | |
Potters Industries A-Series P-0100 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Particle Size | 180 - 350 µm | 180 - 350 µm | |
Micropol Microcoat DG/EVA/214A Microground modified EVA copolymer Specially developed for high specification coating where metal/coating adhesion is of primary importance. Typically used on large flat surfaces, and when toughness, elasticity and excellent barrier .. |
|||
Particle Size | 180 - 200 µm | 180 - 200 µm | |
Lucite International Elvacite ® 2010 Acrylic Resin Elvacite® 2010 is a medium molecular weight methyl methacrylate polymer. 2010 is excellent for use as a general purpose grade for lacquer coatings, such as barrier topcoats for vinyl. It provides.. |
|||
Particle Size | 180 µm | 180 µm | 95% min, 80 mesh; TI-2087 |
Solvay RHODICARE CFT Surfactant Description: Rhodicare® CFT is Cellulase-free clear grade of Xanthan Gum, it is recommended when associated with cellulose-based polymers. Approved for Ecocert. It is excellent anionic bio-polyme.. |
|||
Particle Size | 180 µm | 180 µm | 95 min, 80 mesh; TI-2087 |
Solvay RHODICARE T Surfactant Description: Rhodicare® T is high purity grade specifically designed for thickening and suspension in clear formulations. It has high electrolyte stability over a wide range of pH and fast hydrat.. |
|||
Particle Size | 180 µm | 180 µm | 95 min, 80 mesh; TI-2087 |
Solvay RHODICARE XC Surfactant Description: Rhodicare® XC is similar to standard Xanthan Gum, this grade displays improved microbial specifications. It has high electrolyte stability over a wide range of pH and fast hydration .. |
|||
Particle Size | <= 180 µm | <= 180 µm | >95%; TI-2087 |
Solvay RHODOPOL® T Surfactant Description: Transparent grade xanthan gum. It is It exhibits high pseudoplastic behavior effective thickening and stabilizing agent.Identification: XANTHAN GUMCAS: 11138 – 66 – 2Available.. |
|||
Particle Size | >= 180 µm | >= 180 µm | d50, 68%, vibrated sieving |
TIMCAL TIMREX® 50X100 mesh FR Natural Flake Graphite TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-.. |
|||
Particle Size | <= 180 µm | <= 180 µm | >95%, Guaranteed |
TIMCAL TIMREX® KS150 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | >= 180 µm | >= 180 µm | 0.2% |
TIMCAL TIMREX® KS150 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | <= 180 µm | <= 180 µm | >95%, Guaranteed |
TIMCAL TIMREX® T150 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | >= 180 µm | >= 180 µm | 0.5% |
TIMCAL TIMREX® T150 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 180 µm | 180 µm | 99.5 min, 80 mesh; TI-2087 |
Solvay RHODICARE H Surfactant Description: Rhodicare® H is an anionic bio-polymer with excellent stabilizing, thickening and suspending properties. It has high electrolyte stability over a wide range of pH and fast hydration ra.. |
|||
Particle Size | 180 µm | 180 µm | 95 min, 80 mesh; TI-2087 |
Solvay RHODICARE S Xanthan Gum Surfactant Rhodicare® S 100% natural thickening biopolymer delivering viscosity and suspension/stabilization properties to cosmetic formulations. Rhodicare® S displays a high hydration rate. Approved for Eco.. |