Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 1.25 - 1.35 g/cc | 0.0452 - 0.0488 lb/in³ | |
Nabaltec GRANALOX® NM 9212 E Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Bulk Density | 1.25 - 1.35 g/cc | 0.0452 - 0.0488 lb/in³ | |
Nabaltec GRANALOX® NM 9216 Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Bulk Density | 1.25 - 1.35 g/cc | 0.0452 - 0.0488 lb/in³ | |
Nabaltec GRANALOX® NM 9612 Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Bulk Density | 1.25 - 1.35 g/cc | 0.0452 - 0.0488 lb/in³ | |
Nabaltec GRANALOX® NM 9620 Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Bulk Density | 1.25 - 1.35 g/cc | 0.0452 - 0.0488 lb/in³ | |
Nabaltec GRANALOX® NM 9622 Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Bulk Density | 1.25 - 1.35 g/cc | 0.0452 - 0.0488 lb/in³ | |
Nabaltec GRANALOX® NM 9816 Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Bulk Density | 1.25 - 1.35 g/cc | 0.0452 - 0.0488 lb/in³ | |
Nabaltec GRANALOX® NM 9923 Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Bulk Density | 1.25 g/cc | 0.0452 lb/in³ | Dried at 110°C |
Sharadaa Ceramics REFINSUL 11 Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |
|||
Bulk Density | 1.25 g/cc | 0.0452 lb/in³ | Dried at 110°C |
Sharadaa Ceramics REFINSUL 11LI Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |
|||
Bulk Density | >= 1.25 g/cc | >= 0.0452 lb/in³ | After Drying at 110°C |
Sharadaa Ceramics ZAP 013 Smart Cast Application Special Properties: Low Density, High Strength, Low Thermal ConductivityIndustry: Multi PurposeApplication: All type furnaces as a back up layer, Insulating Burner BlocksInformation provided by Shar.. |
|||
Bulk Density | >= 1.25 g/cc | >= 0.0452 lb/in³ | |
Chosun Refractories C-3 Insulating Firebrick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |