Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 3.60 - 3.65 g/cc | 0.130 - 0.132 lb/in³ | Sintered Density |
Nabaltec GRANALOX® NM 9216 Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Density | 3.20 - 3.65 g/cc | 0.116 - 0.132 lb/in³ | |