NOVA Chemicals Novapol® PI-2024-A LLDPE Masterbatch Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer NOVA Chemicals
Trade Name Novapol®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Novapol® PI-2024-A LLDPE Masterbatch Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Molded Plaque Properties. Features: easy processing, good ESCR and moldability.Applications: housewares, trash cans, industrial containers, toys.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 0.924 g/cc
0.0334 lb/in³
ASTM D792
Environmental Stress Crack Resistance 150 hour
150 hour
F50, Condition A, ASTM D1693, 100% Igepal
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 190 °C
20 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 12.0 MPa
1740 psi
ASTM D638
Elongation at Break 300 %
300 %
ASTM D638
Modulus of Elasticity 0.310 GPa
45.0 ksi
Secant; ASTM D638
Processing Properties Metric English Comments
Melt Temperature 160 - 230 °C
320 - 446 °F