Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 12.0 MPa | 1740 psi | ISO 527 |
Polimeri Europa Riblene® MP 31 R Low Density Polyethylene - Injection Molding Riblene MP 31 R is a medium fluidity low density polyethylene resin (LDPE), with added slip agent.Parts made by Riblene MP 31 R are characterized by a medium rigidity.Main Applications: Riblene MP .. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | -25% change after 70 hours @ 150°C; ASTM D412 |
Precision Polymer Engineering Z80B Hydrogenated NBR Compound Peroxide cured, Hydrogenated Nitrile Rubber, 75-80 °IRHD. Medium acrylonitrile content (ACN = 33.5%). ASTM designation = HNBR. ASTM D2000 line call-out 4MDH716, A26, B36, EO16, EO36, F14, Z1. Z1 .. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | ASTM D638 |
NOVA Chemicals Novapol® GI-2024-A LLDPE Masterbatch Resin Molded Plaque Properties. Features: Granular; improved dispersion, easy processing, good ESCR.Applications: additives, masterbatches/compounding, housewares, trashcans, containers, toys.Data provid.. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | ASTM D638 |
NOVA Chemicals Novapol® PI-2024-A LLDPE Masterbatch Resin Molded Plaque Properties. Features: easy processing, good ESCR and moldability.Applications: housewares, trash cans, industrial containers, toys.Data provided by the manufacturer. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | 500 mm/min; ASTM D638 |
NOVA Chemicals Sclair® 2114 LLDPE Injection Molding Resin Features: High stiffness, high impact strength and low warpage, good top loading capability, high surface gloss.Applications: Container (tub) lids and closures.Data provided by the manufacturer. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | ASTM D638 |
Petroquimica Triunfo Trithene® TN 7006 LDPE - Coextruded Film The Trithene® TS 7006 resin is a low-density polyethylene (LDPE) with high molecular weight and very good clarity. The unique combination of good processability, bubble stability, gloss, and streng.. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | ISO 527 |
Total Lacqtene® FD 0270 LDPE, blown film, compounding, injection molding
(discontinued **) Low density radical polyethylene made by high pressure process. Temperature profile (°C) for injection molding: 200 to 260Information provided provided by Total Petrochemicals.Total Petrochemicals .. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | ASTM D638 |
Huntsman PE1065 Film Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Yields film with excellent optical and machinability.Applications: Film extrusion: soft goods and other high clarity packaging.FDA Notes: Conforms to FDA regu.. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | ASTM D638 |
Petroquimica Triunfo Trithene® TX 3003 LDPE - Shrink Wrap Film The Trithene® TX 3003 resin is a low-density polyethylene (LDPE) with high molecular weight, presenting excellent mechanical properties. The product provided elevated gloss and transparency, adding.. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | ASTM D638 |
Petroquimica Triunfo Trithene® TX 8024 LDPE - High Clarity Film The Trithene TX 8024 resin is a low-density polyethylene (LDPE) with high molecular weight and distribution narrow, designed to obtain films with very high clarity and excellent processability. This.. |
|||
Tensile Strength, Yield | 12.0 MPa @Temperature 22.0 °C |
1740 psi @Temperature 71.6 °F |
25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® MMC 1600 Unsaturated Polyester UP MMC 1600 is a mineral moulding compound (similar to DMC/BMC) providing of a stone like appearance eg. granite or marble. Chrome plated mould surfaces are required. It is recommended that product thi.. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP UX05504 PPA LNP THERMOCOMP* UX05504 is a compound based on Polyphthalamide resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | 9.8 in/min; ASTM D638 |
Teknor Apex Sinvicomp SIM 5515 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: High Strength Uses: Electrical/Electronic Applications < Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | At 50 mm/min; ISO 527-2 |
Borealis Bormed™ LE6607-PH LDPE for Pharmaceutical Blow Molding Bormed LE6607-PH is a LD-polyethylene produced in a high pressure process intended for blow molding of sot and flexible packages for pharmaceutical products.Bormed LE6607-PH can be used in "blow-fil.. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | MD/TD; ISO 527-3 |
Borealis FG5190 Linear Low Density Polyethylene FG5190 is a Butene Linear Low Density Polyethylene for Film Extrusion. Includes Antioxidant. The grade is developed for medium and heavy duty bags, bags and bin liners, dual stretch films, and film.. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | MD/TD; ISO 527-3 |
Borealis FG5223 Linear Low Density Polyethylene FG5223 is a Butene Linear Low Density Polyethylene for Film Extrusion. Includes antioxidant and anti-block additives. This grade is developed for production of lamination film. FG5223 has good heat.. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | ASTM-D638 |
Polyram RamOfin PPC371B73 Polypropylene, 73% Mineral Filled 73% mineral filled polypropylene for heavy density injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | |
Trelleborg B739 Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | 50 mm/min |
Eastman Ecdel PCCE 9965 Copolyester Ether Elastomer ISO data as provided by the manufacturer, Eastman Chemical |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | 2 in/min, Type IV bar; ASTM D638 |
Chevron Phillips Marlex® K203 LLDPE Sheet Extrusion Resin Type: Hexene CopolymerCharacteristics: Outstanding ESCRBroad fusion rangeExcellent melt strengthGood processabilityExcellent flexibilityImproved output and texturingApplications: Coextruded ca.. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | Across Flow; ASTM D638 |
ExxonMobil Santoprene® 103-50 Thermoplastic Elastomer A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Tensile Strength, Yield | 12.0 MPa @Strain 50.0 % |
1740 psi @Strain 50.0 % |
|
Covestro Texin® 985 Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionBlow moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer Mater.. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | ASTM-D638 |
Braskem EG0921 LDPE Blow Molding Polyethylene EG0921 is a low-density polyethylene with good mechanical properties and environmental stress cracking resistance (ESCR) and excellent sealability. It is used in blow molded parts and medium-resista.. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | ASTM-D638 |
Braskem ML2400N LLDPE Injection Molding Polyethylene The resin ML2400N is a linear low-density polyethylene, 1-butene based, with good flexibility and low warpage. It does not contain a slip agent. It does have narrow molecular weight distribution. Th.. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | ASTM D638 |
Huntsman PE2072 Injection Molding Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Very high flow rapid set-up characteristics, excellent clarity, gloss, and stiffness.Applications: Injection molding: lids and difficult to fill applications... |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | ASTM D638 |
Huntsman PE2075 Injection Molding Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Very high flow rapid set-up characteristics, excellent clarity, and gloss.Applications: Injection molding: lids and difficult to fill applications.FDA Notes: .. |
|||
Tensile Strength, Yield | 12.0 MPa @Strain 50.0 % |
1740 psi @Strain 50.0 % |
|
Covestro Texin® 255 Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adop.. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | |
Trelleborg B643 High Quality Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | |
Trelleborg B644 High Quality Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Tensile Strength, Yield | 12.0 - 117 MPa @Temperature -40.0 - 120 °C |
1740 - 17000 psi @Temperature -40.0 - 248 °F |
Average value: 56.9 MPa Grade Count:8 |
Overview of materials for Nylon 6, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri.. |