Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 12.0 MPa | 1740 psi | ASTM D412 |
Precision Polymer Engineering N75L Nitrile Rubber Nitrile Butadiene Rubber (NBR), 65-75 °IRHD. Ultra-Low acrylonitrile (ACN) content. Copolymer of acrylonitrile and butadiene. To meet ASTM D2000/SAE J200 line call-out: MBF710, B34, F19.Application.. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | -25% change after 70 hours @ 150°C; ASTM D412 |
Precision Polymer Engineering Z80B Hydrogenated NBR Compound Peroxide cured, Hydrogenated Nitrile Rubber, 75-80 °IRHD. Medium acrylonitrile content (ACN = 33.5%). ASTM designation = HNBR. ASTM D2000 line call-out 4MDH716, A26, B36, EO16, EO36, F14, Z1. Z1 .. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | ASTM D 638 |
NOVA Chemicals Novapol® LM-0724-A LDPE Injection Molding Resin LM-0724-A complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food. It is also biolog.. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | ASTM D638 |
Petroquimica Triunfo Trithene® TS 7006 LDPE - Coextruded Film The Trithene TS 7006 resin is a low-density polyethylene (LDPE) with high molecular weight and very good clarity. The unique combination of good processability, bubble stability, gloss, and strength.. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | ASTM D638 |
ExxonMobil Santoprene® 273-50 Thermoplastic Elastomer
(discontinued **) A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | ISO 527 |
Polimeri Europa Riblene® MP 30 Low Density Polyethylene - Injection Molding Riblene MP 30 is a medium fluidity low density polyethylene resin (LDPE).Parts made by Riblene MP 30 are characterized by a medium rigidity.Main Applications: Riblene MP 30 is suitable for injectio.. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | |
Chevron Phillips 7105T LLDPE Sheeting Resin
(discontinued **) Resin Type: Sheeting Resin for the Geomembrane Market; ASTM D 4976 Classification: PE 214, A 35307Applications:Blown Geomembrane Applications, Sanitary Landfill Liners, Waste Water Reservoir Contain.. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | |
Chevron Phillips 7108T LLDPE Sheeting Resin
(discontinued **) Resin Type: Sheeting Resin for the Geomembrane Market; ASTM D 4976 Classification: PE 214, A 35307Applications:Cast Geomembrane Applications, Sanitary Landfill Liners, Waste Water Reservoir Containm.. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | 50% Elongation; ASTM D412 |
Covestro Texin® 5250 Thermoplastic Polyurethane, Polyether-based, Medical
(discontinued **) This grade is in chemical compliance with 21 CFR 177.1680 (Polyurethane Resins) and 177.2600 (Rubber articles intended for repeated use) subject to the limitations of this regulation and any other r.. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | ISO 527 |
Total Lacqtene® FD 0270 LDPE, blown film, compounding, injection molding
(discontinued **) Low density radical polyethylene made by high pressure process. Temperature profile (°C) for injection molding: 200 to 260Information provided provided by Total Petrochemicals.Total Petrochemicals .. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | ASTM D638 |
Huntsman PE5030 Extrusion Coating Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Good draw down, low neck-in, good heat sealability and adhesion, low smoking, and excellent printabilityApplications: Extrusion: coating grade and general coa.. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | ASTM D638 |
Petroquimica Triunfo Trithene® TX 3003 LDPE - Shrink Wrap Film The Trithene® TX 3003 resin is a low-density polyethylene (LDPE) with high molecular weight, presenting excellent mechanical properties. The product provided elevated gloss and transparency, adding.. |
|||
Tensile Strength, Yield | 12.0 - 95.0 MPa | 1740 - 13800 psi | Average value: 59.4 MPa Grade Count:5 |
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are incl.. |
|||
Tensile Strength, Yield | 12.0 MPa @Temperature 22.0 °C |
1740 psi @Temperature 71.6 °F |
25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® MMC 1600 Unsaturated Polyester UP MMC 1600 is a mineral moulding compound (similar to DMC/BMC) providing of a stone like appearance eg. granite or marble. Chrome plated mould surfaces are required. It is recommended that product thi.. |
|||
Tensile Strength, Yield | 12.0 MPa @Strain 0.200 %, Temperature 1150 °C |
1740 psi @Strain 0.200 %, Temperature 2100 °F |
|
Haynes 214® alloy, cold rolled annealed sheet 2.0-3.2 mm thick Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | ASTM D412 |
Teknor Apex APEX® 90-A472R-70-NT Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Medical Applications, Caps, Closures, Valves/Valve Parts Appearance-ClearForms-PelletsProcessing Method-.. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP UX05504 PPA LNP THERMOCOMP* UX05504 is a compound based on Polyphthalamide resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP 9H1100C LNP* Thermocomp* 9H1100C is a High Specific Gravity compound containing proprietary fillers. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | 9.8 in/min; ASTM D638 |
Teknor Apex Sinvicomp SIM 5515 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: High Strength Uses: Electrical/Electronic Applications < Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | At 50 mm/min; ISO 527-2 |
Borealis Bormed™ LE6607-PH LDPE for Pharmaceutical Blow Molding Bormed LE6607-PH is a LD-polyethylene produced in a high pressure process intended for blow molding of sot and flexible packages for pharmaceutical products.Bormed LE6607-PH can be used in "blow-fil.. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | MD/TD; ISO 527-3 |
Borealis FG5224 Linear Low Density Polyethylene FG5224 is a Butene Linear Low Density Polyethylene for Film Extrusion. Includes antioxidant, anti-block and medium slip additives. This grade is developed for production of lamination film. FG5224 .. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | ISO R527 |
Total FE 8000 LDPE blown film Low density radical polyethylene made by high pressure autoclave. Advised temperature profile : 160 to 200°C.Information provided provided by Total Petrochemicals.Total Petrochemicals acquired form.. |
|||
Tensile Strength, Yield | 12.0 MPa @Strain 50.0 % |
1740 psi @Strain 50.0 % |
|
Covestro Texin® 4210 Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience w.. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | Across Flow; ASTM D638 |
ExxonMobil Santoprene® 103-50 Thermoplastic Elastomer A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Tensile Strength, Yield | 12.0 MPa @Strain 50.0 % |
1740 psi @Strain 50.0 % |
|
Covestro Texin® 985 Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionBlow moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer Mater.. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | ASTM D638 |
Arkema Group Pebax® 5533 Polyether Block Amide (PEBA) Information provided by Arkema Group |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | ASTM-D638 |
Braskem LD5000A LDPE Blow Molding Polyethylene LD5000A is a low-density polyethylene with good mechanical properties, good ESCR, and excellent sealing characteristics. It does not contain additives. It is used in general purpose blow molded arti.. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | ISO R 527 |
Addiplast Addilene H 420 K24 Polypropylene Homopolymer High densityInformation provided by Addiplast. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | ASTM D638 |
Huntsman PE2062 Injection Molding Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: High flow characteristics combined with good glossApplications: Injection molding: large moldings including housewares and toys.FDA Notes: Conforms to FDA reg.. |
|||
Tensile Strength, Yield | 12.0 - 117 MPa @Temperature -40.0 - 120 °C |
1740 - 17000 psi @Temperature -40.0 - 248 °F |
Average value: 56.9 MPa Grade Count:8 |
Overview of materials for Nylon 6, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri.. |