Material Notes:
This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved thermal resistance.Applications: This grade is used for medium density foam with improved thermal resistance. Typical applications include hot water insulation and automotive parts (interior and exterior).Processing of DYTHERM beads on pressurized batch pre-expanders is recommended. DYTHERM 140R can be processed on a continuous pre-expander when high densities are acceptable. Detailed processing advice is given in the DYTHERM bulletins, available from your local NOVA Chemicals company.This grade should not be used for food contact applications.Information provided by NOVA Chemicals.
Physical Properties Metric English Comments
Bulk Density 0.620 g/cc
0.0224 lb/in³
Density >= 0.0200 g/cc
>= 0.000723 lb/in³
Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure
0.0200 - 0.100 g/cc
0.000723 - 0.00361 lb/in³
Normal molded density assuming cost optimized selection of processing conditions.
Bead Size 1.00 - 1.50 mm
0.0394 - 0.0591 in
0.900 - 1.60 mm
0.0354 - 0.0630 in
Breda Laboratory Analytical Methods 90.30
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 104 °C
219 °F
Modified ISO 2796-1980; Typical maximum temperature to which parts can be exposed short term (1 hour) without significant deformation (<1%).
Chemical Properties Metric English Comments
Styrene Content <= 0.10 %
<= 0.10 %
Residual Styrene Monomer Content per Breda Laboratory Analytical Methods 90.16
Blowing Agent Content >= 5.7 %
>= 5.7 %
Breda Laboratory Analytical Methods 90.18