Physical Properties | Metric | English | Comments |
---|---|---|---|
Bead Size | 0.900 - 1.60 mm | 0.0354 - 0.0630 in | Breda Laboratory Analytical Methods 90.30 |
NOVA Chemicals Dytherm® 140R Expandable Polystyrene This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma.. |
|||
Bead Size | 0.900 - 1.60 mm | 0.0354 - 0.0630 in | Breda Laboratory Analytical Methods 90.30 |
NOVA Chemicals Dytherm® 240R Expandable Polystyrene This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma.. |
|||
Bead Size | 0.900 - 1.60 mm | 0.0354 - 0.0630 in | Breda Laboratory Analytical Methods 90.30 |
NOVA Chemicals Dytherm® 340R Expandable Polystyrene This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma.. |
|||
Bead Size | 1.00 - 1.60 mm | 0.0394 - 0.0630 in | |
IRPC Polimaxx Pentfoam 255E Expandable Polystyrene General: Pentfoam 255E is a self extinguishing grade expandable polystyrene containing pentane as blowing agent. This grade is developed to meet the demand for fast expansion rate and short pressure.. |
|||
Bead Size | 0.800 - 1.60 mm | 0.0315 - 0.0630 in | |
IRPC Polimaxx Pentfoam 291L Expandable Polystyrene General: Pentfoam 291L is a regular grade expandable polystyrene containing pentane as blowing agent. This grade is developed to meet the demand for fast molding cycles in vacuum machine.Application.. |