Polymer Property : Bead Size = 1.60 mm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bead Size 0.900 - 1.60 mm
0.0354 - 0.0630 in
Breda Laboratory Analytical Methods 90.30
NOVA Chemicals Dytherm® 140R Expandable Polystyrene
This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma..
Bead Size 0.900 - 1.60 mm
0.0354 - 0.0630 in
Breda Laboratory Analytical Methods 90.30
NOVA Chemicals Dytherm® 240R Expandable Polystyrene
This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma..
Bead Size 0.900 - 1.60 mm
0.0354 - 0.0630 in
Breda Laboratory Analytical Methods 90.30
NOVA Chemicals Dytherm® 340R Expandable Polystyrene
This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma..
Bead Size 1.00 - 1.60 mm
0.0394 - 0.0630 in
IRPC Polimaxx Pentfoam 255E Expandable Polystyrene
General: Pentfoam 255E is a self extinguishing grade expandable polystyrene containing pentane as blowing agent. This grade is developed to meet the demand for fast expansion rate and short pressure..
Bead Size 0.800 - 1.60 mm
0.0315 - 0.0630 in
IRPC Polimaxx Pentfoam 291L Expandable Polystyrene
General: Pentfoam 291L is a regular grade expandable polystyrene containing pentane as blowing agent. This grade is developed to meet the demand for fast molding cycles in vacuum machine.Application..