Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PlastxWorld Veroplas PB2000 Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced
Manufacturer PlastxWorld, Inc.
Trade Name Veroplas
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastxWorld Veroplas PB2000 Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
general purpose, unfilled injection molding gradeInformation provided by PlastxWorld Inc.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM A792
Moisture Absorption at Equilibrium <= 0.17 %
<= 0.17 %
Karl Fischer
Linear Mold Shrinkage 0.028 cm/cm
0.028 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 75.2 MPa
10900 psi
ASTM D638
Elongation at Break 20 %
20 %
ASTM D638
Flexural Yield Strength 90.3 MPa
13100 psi
ASTM D790
Flexural Modulus 2.90 GPa
421 ksi
ASTM D790
Izod Impact, Notched 0.400 J/cm
0.750 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °C
180 °F
ASTM D648
Vicat Softening Point 199 °C
390 °F
ASTM D1525
Glow Wire Test 649 °C
1200 °F
UNE 20-672-83
Users viewing this material also viewed the following: