Physical Properties | Metric | English | Comments |
---|---|---|---|
Bead Size | 1.00 - 1.50 mm | 0.0394 - 0.0591 in | |
NOVA Chemicals Dytherm® 140R Expandable Polystyrene This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma.. |
|||
Bead Size | 1.00 - 1.50 mm | 0.0394 - 0.0591 in | |
NOVA Chemicals Dytherm® 240R Expandable Polystyrene This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma.. |
|||
Bead Size | 1.00 - 1.50 mm | 0.0394 - 0.0591 in | |
NOVA Chemicals Dytherm® 340R Expandable Polystyrene This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma.. |
|||
Bead Size | 1.20 - 1.50 mm | 0.0472 - 0.0591 in | |
BASF Neopor® P 5200 Expandable Polystyrene Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane).Remarks: For the production of silver-gray foams having a considerably higher ther.. |