Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NIZHNEKAMSKNEFTEKHIM PP 4240G (EP2S29B) Propylene and Ethylene Copolymer

Category Polymer , Thermoplastic , Polyethylene (PE) , Polypropylene (PP)
Manufacturer NIZHNEKAMSKNEFTEKHIM Inc
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NIZHNEKAMSKNEFTEKHIM PP 4240G (EP2S29B) Propylene and Ethylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when PP is produced, processed and PP-made articles are exploited, effective nucleation, and improved optical properties.Information provided by manufacturer
Physical Properties Metric English Comments
Melt Flow 1.5 - 2.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.5 - 2.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238/L
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 27.0 MPa
>= 3920 psi
ASTM D638
Elongation at Yield >= 11 %
>= 11 %
ASTM D638
Flexural Modulus >= 0.950 GPa
>= 138 ksi
ASTM D790
Izod Impact, Notched >= 0.900 J/cm

@Temperature 23.0 °C
>= 1.69 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Users viewing this material also viewed the following: