NIZHNEKAMSKNEFTEKHIM PE 4115N (16401) Linear Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer NIZHNEKAMSKNEFTEKHIM Inc
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NIZHNEKAMSKNEFTEKHIM PE 4115N (16401) Linear Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Physical Properties Metric English Comments
Density 0.914 - 0.918 g/cc
0.0330 - 0.0332 lb/in³
Base Resin; ASTM D1505
Melt Flow 0.80 - 1.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.80 - 1.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1283/L
24 - 36 g/10 min

@Load 21.6 kg,
Temperature 190 °C
24 - 36 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Flow@21.6kg/Flow@2.16kg ratio < 30; ASTM D1283
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD >= 40.0 MPa
>= 5800 psi
ASTM D882
Film Tensile Strength at Yield, TD >= 32.0 MPa
>= 4640 psi
ASTM D882
Film Elongation at Break, MD >= 700 %
>= 700 %
ASTM D882
Film Elongation at Break, TD >= 800 %
>= 800 %
ASTM D882
Tensile Modulus >= 0.120 GPa
>= 17.4 ksi
MD; ASTM D882
>= 0.130 GPa
>= 18.9 ksi
TD; ASTM D882
Elmendorf Tear Strength, MD >= 6.30 g/micron
>= 160 g/mil
ASTM D1922
Elmendorf Tear Strength, TD >= 15.4 g/micron
>= 390 g/mil
ASTM D1922
Dart Drop Test >= 110 g
>= 0.243 lb
ASTM D1709
Descriptive Properties Value Comments
Gel Content (pcs./m²) 0
> 1mm
245
(0.2-0.5)mm
250
> 0.2mm (totally)
5
(0.5-1.0)mm