Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Flow = 0.80 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 0.80 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.80 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Polimeri Europa Eraclene® BC 86 High Density Polyethylene - Blow Molding
Eraclene BC 86 is a high density polyethylene resin (HDPE) with antioxidants, suitable for blow molding application. It is especially recommended for the production of containers up to 20 liters.Er..
Melt Flow 0.80 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.80 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Polimeri Europa Eraclene® FB 506 Hexene Copolymer High Density Polyethylene - Blown Film Extrusion
Eraclene FB 506 is a high density polyethylene resin (HDPE), hexene copolymer, with antioxidants, suitable for blown film extrusion.Its broad molecular weight distribution and density successfully c..
Melt Flow 0.80 - 1.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.80 - 1.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1283/L
NIZHNEKAMSKNEFTEKHIM PE 4115N (16401) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 0.80 - 1.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.80 - 1.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1283/L
NIZHNEKAMSKNEFTEKHIM PE 4116N (16401) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 0.80 - 1.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.80 - 1.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1283/L
NIZHNEKAMSKNEFTEKHIM PE 4117N (18401) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 0.80 - 1.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.80 - 1.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1283/L
NIZHNEKAMSKNEFTEKHIM PE 5117N (18601) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 0.80 - 1.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.80 - 1.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1283/L
NIZHNEKAMSKNEFTEKHIM PE 5118N (18601) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 0.80 - 1.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.80 - 1.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1283/L
NIZHNEKAMSKNEFTEKHIM PE 4550N (50401M) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 0.80 - 1.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.80 - 1.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1283/L
NIZHNEKAMSKNEFTEKHIM PE 4650N (50401N) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 0.80 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.80 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
EVALCA EVAL® F100 Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
32 mol % Ethylene.Data provided by EVALCA. Applications: Melt phase forming. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produced as a pa..
Melt Flow 0.80 - 1.6 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.80 - 1.6 g/10 min

@Load 4.76 lb,
Temperature 374 °F
±15%
Kazanorgsintez PE2NT26-13 High Density Polyethylene Composite
Production Method: Copolymerization of eythylene at low pressure in presence of complex catalysts using gaseous-phase method. Application: Composition is intended for injection molding processin..
Melt Flow 0.80 g/10 min

@Load 2.20 kg
0.80 g/10 min

@Load 4.86 lb
ASTM D1238
Sumitomo Chemical ESPOLEX® 820 Thermoplastic Elastomer
ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi..
Melt Flow 0.80 - 1.3 g/10 min

@Load 2.16 kg,
Temperature 170 °C
0.80 - 1.3 g/10 min

@Load 4.76 lb,
Temperature 338 °F
Wacker Silicones Geniomer® 140 Silicone TPE
SLM TPSE 140 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phas..
Melt Flow 0.80 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.80 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Total HDPE 2008 SN 60 High Density Polyethylene - Blow Molding
HDPE 2008 SN 60 is a high density polyethylene with very high stiffness and low viscosity. It has been specifically designed for the manufacture of thin walled containers for foodstuffs.HDPE 2008 S..
Melt Flow 0.80 g/10 min

@Load 5.00 kg
0.80 g/10 min

@Load 11.0 lb
ASTM D 1238
Total HT 514 MDPE film
Finathene® HT 514 is a medium density polyethylene produced by the slurry loop low pressure polymerization process. Finathene® HT 514 can be used alone, blended or coextruded in a wide variety of ..
Melt Flow 0.80 g/10 min

@Load 3.80 kg,
Temperature 230 °C
0.80 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Entec Hylac® EX18 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Melt Flow 0.80 g/10 min

@Load 5.00 kg,
Temperature 200 °C
0.80 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Diamond Polymers ABS 3502E
Description: Extrusion Grade, High ImpactInformation provided by Diamond Polymers, Inc.
Melt Flow 0.80 g/10 min

@Load 5.00 kg,
Temperature 200 °C
0.80 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Diamond Polymers ABS 4003HH
Description: Heat Resistant Grade, Very High HeatInformation provided by Diamond Polymers, Inc.
Melt Flow 0.80 g/10 min

@Load 5.00 kg,
Temperature 200 °C
0.80 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Diamond Polymers ABS 7501 E
Description: Extrusion Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc.
Melt Flow 0.80 g/10 min

@Load 5.00 kg,
Temperature 200 °C
0.80 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Diamond Polymers ABS 7600B
Description: Blow Molding Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc.
Melt Flow 0.80 g/10 min

@Load 5.00 kg,
Temperature 200 °C
0.80 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Diamond Polymers ABS 7600B (ELG)
Description: Blow Molding Grade, Extra High Impact, Low GlossInformation provided by Diamond Polymers, Inc.
Melt Flow 0.80 g/10 min

@Load 5.00 kg,
Temperature 200 °C
0.80 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Diamond Polymers ABS 7602B
Description: Blow Molding Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc.
Melt Flow 0.80 g/10 min

@Load 5.00 kg,
Temperature 200 °C
0.80 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Diamond Polymers ABS 9502E
Description: Extrusion Grade, Ultra High ImpactInformation provided by Diamond Polymers, Inc.
Melt Flow 0.80 g/10 min

@Load 5.00 kg,
Temperature 200 °C
0.80 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Diamond Polymers ABS/PC 9901
Description: Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc.
Melt Flow 0.80 g/10 min

@Load 5.00 kg,
Temperature 200 °C
0.80 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Diamond Polymers ABSPC 9901 ELG ABS/PC Injection Molding Grade, Very High Impact
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Melt Flow 0.80 g/10 min

@Load 5.00 kg,
Temperature 200 °C
0.80 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Diamond Polymers ASA S950
Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc.
Melt Flow 0.80 g/10 min

@Load 5.00 kg,
Temperature 200 °C
0.80 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Diamond Polymers ASA TW-17
Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc.
Melt Flow 0.80 g/10 min

@Load 5.00 kg,
Temperature 200 °C
0.80 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Diamond Polymers ABS 3501 GF-20
Description: Reinforced Grade, 20%Glass FilledInformation provided by Diamond Polymers, Inc.
Melt Flow 0.80 g/10 min

@Load 5.00 kg
0.80 g/10 min

@Load 11.0 lb
ISO 1133
Total Lacqtene® 6002 FLG 42 HDPE film  (discontinued **)
LACQTENE® 6002 FLG 42 is a medium density polyethylene resin with hexene as comonomer. This shows a broad molecular weight distribution ensuring outstanding processability. LACQTENE® 6002 FLG 42 h..
Melt Flow 0.80 g/10 min

@Load 5.00 kg,
Temperature 200 °C
0.80 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Diamond Polymers ABS 3500B
Description: Blow Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc.
Copyright © lookpolymers.com All Rights Reserved