Physical Properties Metric English Comments
Density 0.914 - 0.918 g/cc
0.0330 - 0.0332 lb/in³
Base Resin; ASTM D1505
NIZHNEKAMSKNEFTEKHIM PE 4115N (16401) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Density 0.914 - 0.918 g/cc
0.0330 - 0.0332 lb/in³
Base Resin; ASTM D1505
NIZHNEKAMSKNEFTEKHIM PE 4116N (16401) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Density 0.914 - 0.918 g/cc
0.0330 - 0.0332 lb/in³
Base Resin; ASTM D1505
NIZHNEKAMSKNEFTEKHIM PE 4116P (16402) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Density 0.914 - 0.918 g/cc
0.0330 - 0.0332 lb/in³
Base Resin; ASTM D1505
NIZHNEKAMSKNEFTEKHIM PE 4116Q (16403) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Density 0.914 - 0.918 g/cc
0.0330 - 0.0332 lb/in³
Base Resin; ASTM D1505
NIZHNEKAMSKNEFTEKHIM PE 4115P (16402) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Density 0.914 - 0.980 g/cc
0.0330 - 0.0354 lb/in³
Average value: 0.945 g/cc Grade Count:71
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade". Each property range of values reported ..
Density 0.914 g/cc
0.0330 lb/in³
ASTM D1505
ICO Polymers ICOFLOâ„¢ 510-5049 400 Micron LDPE Powder
Description: ICOFLO 510-5049 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma..
Density 0.914 g/cc
0.0330 lb/in³
ASTM D1505
ICO Polymers ICOFLOâ„¢ 510-5050 500 Micron LDPE Powder
Description: ICOFLO 510-5050 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma..
Density 0.914 g/cc
0.0330 lb/in³
ASTM D1505
ICO Polymers ICOFLOâ„¢ 510-5051 800 Micron LDPE Powder
Description: ICOFLO 510-5051 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma..
Density 0.914 g/cc
0.0330 lb/in³
ASTM D1505
ICO Polymers ICOFLOâ„¢ 510-5052 1200 Micron LDPE Powder
Description: ICOFLO 510-5052 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in m..
Density 0.914 g/cc
0.0330 lb/in³
ASTM D1505
ICO Polymers ICOTEXâ„¢ 520-5016 300 Micron LDPE Powder
Description: ICOTEX 520-5016 is a low density polyethylene powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: good melt flow and a ..
Density 0.914 g/cc
0.0330 lb/in³
ASTM D1505
ICO Polymers ICOTEXâ„¢ 520-5050 500 Micron LDPE Powder
Description: ICOTEX 520-5050 is a low density polyethylene powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: good melt flow and fa..
Density 0.914 g/cc
0.0330 lb/in³
Silon Tabond 3045 Adhesive Resin
TABOND 3045 is LLDPE modified with maleic anhydride functional groups which promote bonding with different materials like polar polymers, metals and surface treated glass.Characteristics: • Str..
Density 0.914 g/cc
0.0330 lb/in³
ASTM D1505
Chevron Phillips MarFlex® D163 Metallocene Linear Low Density Polyethylene, Blown Film
This mLLDPE is tailored for applications that require:Excellent clarityExcellent glossExcellent toughnessExcellent heat sealTypical blown film applications include:Seal layer in coextrusionsHeavy du..
Density 0.914 g/cc
0.0330 lb/in³
ASTM D792, ISO 1183
DuPont™ Appeel® 45D747 Polyolefin
Appeel® 45D747 is a modified polyolefin resin designed to provide easy peel functionality from polyethylene copolymers. Appeel® 45D747 is available in pellet form for use in conventional extrusion..
Density 0.914 g/cc
0.0330 lb/in³
ExxonMobil method
ExxonMobil LDPE LD 650 Low Density Polyethylene Resin (European Grade)
Product Description: LD 650 is an easy flowing LDPE grade with a good flexibility and excellent toughness.Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: NoSlip: No..
Density 0.914 g/cc
0.0330 lb/in³
ASTM D792
Dow ELITE™ 5500G Enhanced Polyethylene Resin
™ 5500G is a copolymer produced via INSITE™ Technology. It offers an exceptional combination of processability, low heat seal initiation temperature, package integrity, optical properties, and te..
Density 0.914 g/cc

@Temperature 23.0 °C
0.0330 lb/in³

@Temperature 73.4 °F
ISO 1183
Arkema Group OREVAC® 18360 Maleic Anhydride Modified Polyethylene
OREVAC® 18360 is anhydride modified polyethylene. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. OREVAC® 1..
Density 0.914 g/cc

@Temperature 0.000 °C
0.0330 lb/in³

@Temperature 32.0 °F
Akzo Nobel Trigonox® 121 Polymerization Initiator
Initiator for the (co)polymerization of ethylene, styrene, acrylates and methacrylates.Information provided by Akzo Nobel Polymer Chemicals.
Density 0.914 g/cc
0.0330 lb/in³
BASF Lupragen® N 400 Trimethylamineoethylethanolamine
Formula: C7H18N2OCAS: 2212-32-0Description: Trimethylaminoethylethanolamine is a colorless to light yellow liquid, with an amine-like odor. It is miscible with water and other organic solvents.Syno..
Density 0.914 g/cc
0.0330 lb/in³
BASF N-Ethylethanolamine
Formula: C4H11NOCAS: 110-73-6Description: N-Ethylethanolamine is a colorless to yellow liquid with an amine-like odor. It is miscible in water.Synonyms: EEA, 2-Ethylaminoethanol, 2-(Ethylamino)etha..
Density 0.914 g/cc
0.0330 lb/in³
ASTM D1505
Huntsman Rexell® V8403 Cast Film Extrusion LLDPE  (discontinued **)
Linear-low very low density copolymer, blown film extrusion, FDA compliantFeatures: Excellent resistance to impact, puncturing, tearing, and flex cracking with good weld seal strength, hot tack, and..
Density 0.914 g/cc
0.0330 lb/in³
ASTM D1505
Huntsman Rexell® V3101 Blown Film Extrusion LLDPE  (discontinued **)
Linear-low very low density copolymer, cast film extrusion, FDA compliant.Features: High toughness, puncture resistance with good sealing and excellent optical properties.Applications: Food packagin..
Density 0.914 g/cc
0.0330 lb/in³
ConocoPhillips 32 Spectrum Cutting Oil
Description: Conoco Spectrum Cutting Oil is a multifunctional cutting fluid formulated with a sulfurized base oil, is a balanced additive system and is suited for a wide variety of machining applica..