Material Notes:
Information provided by Multibase
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
Relative, press-cured
Viscosity 60000 cP
60000 cP
initial; ASTM D1084
110000 cP
110000 cP
after 2 hours; ASTM D1084
115000 cP
115000 cP
base viscosity; ASTM D1084
Mechanical Properties Metric English Comments
Hardness, Shore A 30
30
cured
Tensile Strength, Ultimate 5.03 MPa
730 psi
cured; ASTM D412
Elongation at Break 470 %
470 %
cured; ASTM D412
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+15 ohm-cm
2.00e+15 ohm-cm
ASTM D257
Surface Resistance >= 7.00e+16 ohm
>= 7.00e+16 ohm
ASTM D257
Dielectric Constant 3.0

@Frequency 1000 Hz
3.0

@Frequency 1000 Hz
ASTM D150
3.01

@Frequency 1000 Hz
3.01

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 22.6 kV/mm
575 kV/in
ASTM D149
Dissipation Factor 0.00090

@Frequency 100 Hz
0.00090

@Frequency 100 Hz
ASTM D150
0.0010

@Frequency 100000 Hz
0.0010

@Frequency 100000 Hz
ASTM D150