Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | >= 7.00e+16 ohm | >= 7.00e+16 ohm | ASTM D257 |
Multibase SILASTIC® MDX4-4210 Dow-Corning Biomedical Grade Elastomer Information provided by Multibase |
|||
Surface Resistance | 7.00e+16 ohm | 7.00e+16 ohm | IEC 60093 |
Polyplastics Duranex® 2000 Polybutylene Terephthalate (PBT), High flow DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Surface Resistance | 7.00e+16 ohm | 7.00e+16 ohm | IEC 60093 |
Polyplastics FR-PET® BN3030SD Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Flame retardant, General purpose Information provided by PolyPlastics. |
|||
Surface Resistance | 7.00e+16 ohm | 7.00e+16 ohm | IEC 60093 |
Polyplastics FR-PET® CN3030SD Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Flame retardant, General purpose Information provided by PolyPlastics. |