Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 30 PHR N330 (HAF) Filler

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 30 PHR N330 (HAF) Filler.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear strength, oil and fuel resistance, and ozone resistance. The life expectancy of urethane is often 5 times longer than other elastomers, thus saving material costs and downtime expense. One shortcoming of polyurethanes is loss of physical properties at temperatures over 180°F (82°C). MILLATHANE HT has overcome this weakness.FormulationMillathane HT100.0Zinc Stearate0.5MBTS4.0MBT2.0THANECURE® ZM1.0Sulfur1.5N330 (HAF)30All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 71
71
Tensile Strength, Yield 24.62 MPa
3571 psi
Elongation at Yield 428 %
428 %
100% Modulus 0.00427 GPa
0.619 ksi
200% Modulus 0.009880 GPa
1.433 ksi
300% Modulus 0.01810 GPa
2.625 ksi
Tear Strength 55.7 kN/m
318 pli
Die C
Taber Abrasion, mg/1000 Cycles 0.080
0.080
H-18, mg loss/rev
Compression Set 64 %

@Temperature 70.0 °C,
Time 79200 sec
64 %

@Temperature 158 °F,
Time 22.0 hour
Processing Properties Metric English Comments
Cure Time 20.0 min

@Temperature 149 °C
0.333 hour

@Temperature 300 °F