Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 115000 cP | 115000 cP | base viscosity; ASTM D1084 |
Multibase SILASTIC® MDX4-4210 Dow-Corning Biomedical Grade Elastomer Information provided by Multibase |
|||
Viscosity | 115000 - 125000 cP @Temperature 25.0 °C |
115000 - 125000 cP @Temperature 77.0 °F |
Uncured |
Permabond TA437 Toughened Acrylic Adhesive PERMABOND TA437 is a single component structural acrylic adhesive designed primarily for bonding metals, ferrites and ceramics. The typical fixture time of TA437 when used with Initiator 41 is 30 –.. |
|||
Viscosity | 115000 - 130000 cP | 115000 - 130000 cP | A |
ITW Plexus Plexusâ„¢ MA555 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low exotherm adhesive able to be used 1" thick.Information provided by Illinois Tool Works. |
|||
Viscosity | 115000 cP | 115000 cP | Melt Viscosity, 260°C, 1500 sec-1; ISO 11443 |
SABIC Innovative Plastics Valox® 4631 PBT (Europe-Africa-Middle East) VALOX 4631 is a 30% glass reinforced, flame retarded PBT injection moulding resin with good electrical properties and excellent mechanical properties. |
|||
Viscosity | 115000 cP | 115000 cP | Dynamic |
Dow Corning 7-3110 Volatile Fluid Hip Emulsion A concentrated emulsion of dimethicone and trisiloxane that is designed to facilitate the rapid development of skin care formulations which contain these emollients. Typical applications include: su.. |
|||
Viscosity | 115000 cP | 115000 cP | Dynamic |
Dow Corning 7-3120 VFP Hip Emulsion A concentrated emulsion of dimethicone and trisiloxane that is designed to facilitate the rapid development of skin care formulations which contain these emollients. Typical applications include: su.. |
|||
Viscosity | 115000 cP @Shear Rate 300 1/s, Temperature 190 °C |
115000 cP @Shear Rate 300 1/s, Temperature 374 °F |
ASTM D3835 |
Advanced Polymer Alloys Alcryn® 2250 UT Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |