Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aremco Corr-Paint™ CP4010 High Temperature Protective Silicone Coating, Aluminum Filled

Category Other Engineering Material , Ceramic/Metallic Coating , Polymer , Thermoset , Silicone
Manufacturer Aremco
Trade Name Corr-Paint™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aremco Corr-Paint™ CP4010 High Temperature Protective Silicone Coating, Aluminum Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Single part, silicone-based, low viscosity, heat-curable, aluminum-filled sealer offering exceptional moisture resistance to 1100°F (593°C).
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
Solids Content 41.6 %
41.6 %
volume
44.2 %
44.2 %
weight
Volatile Organic Compounds (VOC) Content 100 g/l
100 g/l
Viscosity 200 - 600 cP
200 - 600 cP
Mixed Viscosity
Thickness 25.4 microns
1.00 mil
recommended dry film thickness
61.0 microns
2.40 mil
estimated wet film thickness
Storage Temperature 12.8 - 29.4 °C
55.0 - 85.0 °F
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 593 °C
1100 °F
Flash Point >= 100 °C
>= 212 °F
Processing Properties Metric English Comments
Processing Temperature 10.0 - 48.9 °C
50.0 - 120 °F
Application Temperature
Dry Time 1.00 - 2.00 hour
1.00 - 2.00 hour
Touch
2.00 - 4.00 hour
2.00 - 4.00 hour
Handling
1.00 - 24.0 hour
1.00 - 24.0 hour
Recoat
Cure Time 45.0 min

@Temperature 249 °C
0.750 hour

@Temperature 480 °F
>1 Hour Air Set Required Prior to Curing
60.0 min

@Temperature 232 °C
1.00 hour

@Temperature 450 °F
>1 Hour Air Set Required Prior to Curing
Shelf Life 6.00 Month

@Temperature 23.0 °C
6.00 Month

@Temperature 73.4 °F
Descriptive Properties Value Comments
Color Aluminum
Dry Film Coverage ft2/gal 611
at 1 mil
Primer Not Required
Thinner Distilled Water