Multibase Multi-Pro® 5012 C Natural 50% Filler Content Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Multibase
Trade Name Multi-Pro®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Pro® 5012 C Natural 50% Filler Content Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This product is well suited to fabricate non-glossy appliance parts, such as a vacuum cleaner canister. It replaces ABS at favorable cost performance characteristics.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.33 g/cc
0.0480 lb/in³
ASTM D792-91
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
ASTM D955-89
Melt Flow 12 g/10 min
12 g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 13.5 MPa
1960 psi
ASTM D638-95
Elongation at Break 82 %
82 %
ASTM D638-95
Flexural Strength 26.1 MPa
3790 psi
ASTM D790-95
Flexural Modulus 2.069 GPa
300.1 ksi
Method 1, Proc. B; ASTM D-790-95
Izod Impact, Notched 2.30 J/cm
4.31 ft-lb/in
ASTM D256-93a
Gardner Impact 18.9 J
13.9 ft-lb
ASTM D5420-93