Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase Multi-Pro® 2008 X Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Multibase
Trade Name Multi-Pro®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Pro® 2008 X Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Linear Mold Shrinkage 0.011 cm/cm
0.011 in/in
ASTM D955
Melt Flow 9.5 g/10 min
9.5 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 30.3 MPa
4400 psi
ASTM D638
Elongation at Break 30 %
30 %
ASTM D638
Flexural Strength 45.5 MPa
6600 psi
ASTM D790
Flexural Modulus 2.56 GPa
371 ksi
Method I (3 point load), Procedure B); ASTM D790
Izod Impact, Notched 0.320 J/cm
0.600 ft-lb/in
73°F; ASTM D256
Gardner Impact 0.5649 J
0.4167 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 135 °C
275 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
Unannealed; ASTM D648
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved