Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 30.3 MPa
4400 psi
ASTM D638
Multibase Multi-Pro® 2008 X Polypropylene
Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Tensile Strength, Ultimate 30.3 MPa
4400 psi
0.125 in, injection molded, unannealed; ASTM D638
Styron EMERGEâ„¢ 5710 Acrylonitrile Butadiene Styrene (ABS)
EMERGEâ„¢ ABS 5710 advanced resin is an ignition resistant ABS resin with an excellent balance of flow and impact strength. Applications: Monitor Enclosures Surge Protectors and UPS Enclosures ..
Tensile Strength, Ultimate 30.3 MPa
4400 psi
Williams Advanced Alloys WS302 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Tensile Strength, Ultimate 30.3 MPa
4400 psi
ASTM D638
CPC - Vycom POLYCARVE™ Coextruded High Density Sheet (HDPE)
PolyCarve™ thermoplastic engraving sign stock made to permanently resist the destructive outdoor elements, and certain indoor environments. PolyCarve is a high density, UV stabilized polyethylene c..
Tensile Strength, Ultimate 30.3 MPa
4400 psi
ASTM D638
CPC - Vycom SANATEC® Sanitary Cutting Boards High Density Polyethylene
Sanatec is a high density polyethylene specially formulated for the manufacture of quality cutting boards. Sanatec`s special surface finish insures long product life and will not dull knives. Sanate..
Tensile Strength, Ultimate 30.3 MPa
4400 psi
ASTM D638
CPC - Vycom SEABOARD™ GRIP-X™ Slip Resistant High Density Polyethylene (HDPE)
Grip-X is a UV stabilized high density polyethylene (HDPE) sheet formulated to meet demanding conditions of the marine industry. Grip-X is manufactured with a special surface treatment and stipulate..
Tensile Strength, Ultimate 30.3 MPa
4400 psi
after optimum cure
Armstrong A-702 Epoxy Adhesive
Information provided by Ellsworth Adhesives.
Tensile Strength, Ultimate 30.3 MPa
4400 psi
ASTM D638
BCC Products EB 6200 Epoxy Tooling Board
EB6200 is a “grain-free” elevated temperature epoxy modeling material known for its superior surface finish, dimensional stability and the ability to maintain tolerances even after being subjected..
Tensile Strength, Ultimate >= 30.3 MPa
>= 4400 psi
ASTM D638
Bulk Molding Compounds BMC 940 Vinyl Ester Bipolar Plate Material
Bulk Molding Compounds, Inc. is the largest manufacturer of thermoset bulk molding compounds in North America, serving the automotive, appliance, and electrical markets. BMC thermosets are the most ..
Tensile Strength, Ultimate 30.3 - 993 MPa
4400 - 144000 psi
Average value: 206 MPa Grade Count:30
Overview of materials for Vinyl Ester Sheet Molding Compound
This property data is a summary of similar materials in the MatWeb database for the category "Vinyl Ester Sheet Molding Compound". Each property range of values reported is minimum and maximum value..