Multibase Multi-Pro® 0001 Black Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Multibase
Trade Name Multi-Pro®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Pro® 0001 Black Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This product was specially designed for one customer's extrusion application needs. Data is taken from sample material only.Data provided by Multibase.
Physical Properties Metric English Comments
Density 0.9176 g/cc
0.03315 lb/in³
ASTM D792-91
Linear Mold Shrinkage 0.0115 cm/cm
0.0115 in/in
ASTM D955-89
Melt Flow 2.2 g/10 min
2.2 g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 22.3 MPa
3230 psi
ASTM D638-95
Elongation at Break 887 %
887 %
ASTM D638-95
Flexural Strength 23.8 MPa
3450 psi
ASTM D790-95
Flexural Modulus 0.806 GPa
117 ksi
Method 1, Proc. B; ASTM D-790-95
Izod Impact, Notched 1.44 J/cm
2.70 ft-lb/in
ASTM D256-93a
Gardner Impact 29.6 J
21.8 ft-lb
ASTM D5420-93
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 37.0 °C
98.6 °F
ASTM D648-95