Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 23.8 MPa | 3450 psi | ASTM D790-95 |
Multibase Multi-Pro® 0001 Black Polypropylene This product was specially designed for one customer's extrusion application needs. Data is taken from sample material only.Data provided by Multibase. |