Mechanical Properties Metric English Comments
Flexural Strength 23.8 MPa
3450 psi
ASTM D790-95
Multibase Multi-Pro® 0001 Black Polypropylene
This product was specially designed for one customer's extrusion application needs. Data is taken from sample material only.Data provided by Multibase.