Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.806 GPa | 117 ksi | Method 1, Proc. B; ASTM D-790-95 |
Multibase Multi-Pro® 0001 Black Polypropylene This product was specially designed for one customer's extrusion application needs. Data is taken from sample material only.Data provided by Multibase. |