Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase Multi-Flex® TPO D 5302 E MB

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO)
Manufacturer Multibase
Trade Name Multi-Flex® TPO
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPO D 5302 E MB.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Multibase.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
ASTM D955-89
Melt Flow 1.0 g/10 min
1.0 g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Hardness, Shore D 53
53
10 sec; ASTM D-2240-95
Tensile Strength, Ultimate 22.4 MPa
3250 psi
ASTM D638-95
Elongation at Break 630 %
630 %
ASTM D638-95
Flexural Strength 17.4 MPa
2520 psi
ASTM D790-95
Flexural Modulus 0.690 GPa
100 ksi
Secant 1%; ASTM D-790-95
Izod Impact, Notched NB
NB
ASTM D-256-93a
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 73.0 °C
163 °F
ASTM D648-95
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved