Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 73.0 °C @Thickness 3.18 mm |
163 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Maxxam™ FR PP FR 7B31 Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.0 °C | 163 °F | ASTM D648-95 |
Multibase Multi-Flex® TPO D 5302 E MB Data provided by Multibase. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.0 °C | 163 °F | ASTM D648 |
Formosa Plastics Formolene® HL4506 Blow Molding HDPE
(discontinued **) Extra High Molecular Weight Hexene CopolymerApplications: Multi-layer fuel tanks, mono-layer fuel tanks, industrial bulk containers (IBC)Formolene HL4506 is intended for large part blow molding appl.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.0 °C | 163 °F | |
LyondellBasell Lupolen® 5231 HX HDPE, Impact Grade Medium flow, impact resistant, very stress-crack resistant grade for closures, bottles that contain carbonated liquids, storage and tote boxes, as well as engineering components.Data was collected b.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 72.8 °C | 163 °F | ASTM D648 |
LyondellBasell Alathon® H5220 High Density Polyethylene, Injection Molding Grade ApplicationsAlathon H5220 provides easy processing characteristics and exhibits excellent toughness properties and color as well as low odor and good processing stability. Typical applications inclu.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 72.8 °C | 163 °F | Unannealed; ASTM D648 |
Global PP-2800-J Polypropylene Block Copolymer Description-opacity, medium to high stiffness, high impact strength at low temperatureApplications-automotive (interior & exterior), cratesInformation provided by Global Polymers Corporation. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.0 °C | 163 °F | ASTM D648 |
LyondellBasell Astryn BA16G Polypropylene Copolymer Key Features: fractional melt flow, medium modulus, UV-stabilized, extrusion grade polypropylene copolymer, good flexibility, high impact strength, good colorability, good processability, good weath.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.0 °C | 163 °F | ASTM D648 |
Lubrizol Stat-Rite® S-250 Static Control Polypropylene Stat-Rite® S-250 is a static dissipative Polypropylene alloy. Stat-Rite S-250 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD pr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.0 °C | 163 °F | ISO 75-2 |
Borealis BorPURE™ RJ377MO Polypropylene, Transparent Random Copolymer BorPure™ RJ377MO is a specially modified high MFR transparent polypropylene random copolymer based on proprietary Borealis Nucleation Technology (BNT), with an excellent organoleptic performance. N.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.0 °C | 163 °F | ASTM D648 |
Eastman DURASTAR DS1010 Natural PCTA Copolyester DURASTAR DS1010 polymer contains a mold release. It has excellent appearance and clarity. Its most outstanding features are chemical resistance and excellent processing characteristics. Exposure to .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.0 °C | 163 °F | ASTM D648 |
Eastman DURASTAR DS2010 Natural PCTA Copolyester DURASTAR DS2010 polymer contains a mold release. It has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing cha.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.0 °C | 163 °F | ASTM D648 |
Eastman DuraStar DS2110UVI Polymer, Natural Durastar DS2110UVI polymer, contains an ultraviolet light stabilization package. It is recommended for indoor applications requiring enhanced color stability upon extended exposure to fluorescent li.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.0 °C | 163 °F | ISO 75 |
Eastman DuraStar MN621 Polymer, Natural Durastar Polymer MN621 was developed for the medical device industry and contains a mold release It processes easily and requires minimal drying time. It has superior toughness, high clarity and goo.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.0 °C | 163 °F | ASTM D648 |
Eastman DuraStar MN621 Polymer, Natural Durastar Polymer MN621 was developed for the medical device industry and contains a mold release It processes easily and requires minimal drying time. It has superior toughness, high clarity and goo.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.0 °C | 163 °F | ASTM D648 |
Eastman DuraStar MN630 Polymer, Natural Durastar Polymer MN630 has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing characteristics. MN630 has very .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.0 °C | 163 °F | ASTM D648 |
Eastman DuraStar MN631 Polymer, Natural Durastar Polymer MN631 contains a mold release. It has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing char.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.0 °C | 163 °F | ASTM D648 |
Eastman Eastar AN014 Copolyester Eastar AN014 copolyester is a high flow product that contains a mold release. Eastar AN014 flow lengths are increased 20-40% relative to Eastar AN004 as shown by spiral flow testing. Other outstandi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.0 °C | 163 °F | ASTM D648 |
Eastman Eastar BR001 Copolyester Eastar BR001 Copolyester has excellent appearance and is nearly water-clear. Its most outstanding features are its chemical resistance and processing capabilities. Exposure to aromatic oils often ca.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.0 °C | 163 °F | ASTM D648 |
Eastman Eastar BR203 Copolyester Eastar BR203 Copolyester contains a mold release additive. It has excellent appearance and is nearly water-clear. Its most outstanding features are its chemical resistance and processing capabilitie.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.0 °C | 163 °F | |
Eastman Eastar DN001 PCTG Copolyester ISO data as provided by the manufacturer, Eastman Chemical |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.0 °C | 163 °F | ASTM D648 |
Eastman Eastar DN010 Copolyester Eastar Copolyester DN010 is a brilliantly clear polymer having excellent impact strength, chemical resistance, and low shrinkage rates. Eastar Copolyester DN010 contains no mold release.Applications.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.0 °C | 163 °F | ASTM D648 |
Eastman Eastar DN011 Copolyester Eastar Copolyester DN011 is a brilliantly clear polymer having excellent impact strength, chemical resistance, and low shrinkage rates. Eastar Copolyester DN011 contains a mold release.Applications/.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.0 °C | 163 °F | ASTM D648 |
Eastman Eastar EB062 Copolyester Eastar Copolyester EB062 is a resin specifically developed for extrusion blown bottles where aesthetics such as high clarity and gloss, coupled with design flexibility, drive demand. Compared to com.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.0 °C | 163 °F | ASTM D648 |
Eastman Eastar MB002 Copolyester Eastar copolyester MB002 is a resin specifically developed for extrusion blow molding containers in medical applications where aesthetics such as high clarity and gloss, coupled with high toughness .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.0 °C | 163 °F | ASTM D648 |
Eastman Provista MP002 Copolymer Provista Copolymer MP002 is a resin specifically developed for extrusion into profiles for medical applications where aesthetics such as high clarity and gloss, coupled with design flexibility and e.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 72.8 °C | 163 °F | Molded and tested in accordance with ASTM D4976; ASTM D648 |
Dow DMDA-8907 NT 7 High Density Polyethylene Resin DOW DMDA-8904 NT 7 is produced using UNIPOL™ process technology. It is intended for use in injection molding applications such as pails, industrial parts and other shipping containers. Information.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.0 °C | 163 °F | ASTM D648 |
Eastman Eastar GN078 Copolyester, Natural Eastar Copolyester GN078 builds on the strength of Eastar Copolyester GN077 by offering improved melt strength and toughness. Eastar Copolyester GN078 does not meet FDA compliance but is an excellen.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.0 °C | 163 °F | |
BASF Novolen® 2300 L Polypropylene Injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 72.8 °C | 163 °F | ASTM D648 |
Aaron Industries AAROLENE® ARPE LD 300-1 Low Density Polyethylene Compounded Resin AAROLENE® ARPE 300 Series Polyethylene Compounded Resin LDPEColor may be specified. Melt Flow Index may be specified. Specific Gravity may be specified. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.0 °C | 163 °F | |
Arkema Group Rilsan® 8020 Nylon 11, Flexible Tubing Grade (Conditioned) Designation ISO 1874-PA11/xx,E,16-003Transparent and flexible copolymer for tubes extrusion. Additive free.Good flexibility. Very good transparency. High chemical resistance.USP XXIII class VI appro.. |