Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase Multi-Flex® TPE A 9103 BLK

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Multibase
Trade Name Multi-Flex® TPE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPE A 9103 BLK.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0096 cm/cm
0.0096 in/in
ASTM D955
Melt Flow 4.0 g/10 min
4.0 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 87
87
10 sec; ASTM D-2240
Tensile Strength, Ultimate 9.00 MPa
1310 psi
ASTM D412
Elongation at Break 700 %
700 %
ASTM D412
Flexural Modulus 0.121 GPa
17.5 ksi
method 1, Proc.B; ASTM D-790
Tear Strength 52.5 kN/m
300 pli
ASTM D624