Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.121 GPa | 17.5 ksi | method 1, Proc.B; ASTM D-790 |
Multibase Multi-Flex® TPE A 9103 BLK Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Flexural Modulus | 0.121 GPa | 17.5 ksi | 1% Secant; ASTM D790 |
Entec Hypel® PELD12/.920 LDPE
(discontinued **) Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Flexural Modulus | 0.121 GPa | 17.5 ksi | ASTM D790 |
LyondellBasell Microthene® G MN70100 Low Density Polyethylene General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique prop.. |
|||
Flexural Modulus | 0.121 GPa | 17.6 ksi | ASTM D790 |
LyondellBasell Microthene® G MN71020 Low Density Polyethylene General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique prop.. |
|||
Flexural Modulus | 0.121 GPa | 17.6 ksi | ASTM D790 |
LyondellBasell Microthene® G MN71120 Low Density Polyethylene (Rotomolding) General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique prop.. |
|||
Flexural Modulus | 0.121 GPa | 17.5 ksi | ASTM D790 |
LyondellBasell Microthene® G MN71400 Low Density Polyethylene General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique prop.. |