Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0096 cm/cm
0.0096 in/in
ASTM D955
Multibase Multi-Flex® TPE A 8502-SR BLK
Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Linear Mold Shrinkage 0.0096 cm/cm
0.0096 in/in
ASTM D955
Multibase Multi-Flex® TPE A 9103 BLK
Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.