Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Borealis FA3220 Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer Borealis
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis FA3220 Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FA3220 is a Low Density Polyethylene for Film Extrusion. Autoclave Technology. Unmodified. This grade is developed to give a strong film with balanced shrink properties. Applications FA3220 has been developed especially for applications like: heavy-duty sack, food packaging, agricultural films, construction films, and shrink film.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.922 g/cc
0.0333 lb/in³
ISO 1183
Melt Flow 0.30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 400 %
400 %
ISO 527-3
Film Elongation at Break, TD 600 %
600 %
ISO 527-3
Tensile Modulus 0.190 GPa
27.6 ksi
MD/TD; ASTM D882-A
Puncture Energy 5.00 J
3.69 ft-lb
130 N; 125µm sample; ASTM D5748
Coefficient of Friction 0.60
0.60
Dynamic; ISO 8295
Elmendorf Tear Strength, MD 4.077 g/micron
103.6 g/mil
ISO 6383/2
Elmendorf Tear Strength, TD 4.89 g/micron
124 g/mil
ISO 6383/2
Dart Drop Test 450 g
0.992 lb
ISO 7765-1
Film Tensile Strength at Break, MD 25.0 MPa
3630 psi
ISO 527-3
Film Tensile Strength at Break, TD 23.0 MPa
3340 psi
ISO 527-3
Thermal Properties Metric English Comments
Melting Point 110 °C
230 °F
ISO 11357-3
Vicat Softening Point 96.0 °C
205 °F
ISO 306
Processing Properties Metric English Comments
Melt Temperature 170 - 200 °C
338 - 392 °F
Copyright © lookpolymers.com All Rights Reserved