Momentive Performance Materials RTV5249 Neutral Cure, One Component RTV Adhesive Sealant

Category Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Adhesive/Sealant Grade
Manufacturer Momentive Performance Materials (Former GE Silicones)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Momentive Performance Materials RTV5249 Neutral Cure, One Component RTV Adhesive Sealant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
RTV5240 series sealants are alkoxy neutral cure, one-component, ready to use, electronic grade silicone adhesive sealants exhibiting high strength that will maintain a strong bond even when exposed to moist environments. RTV5240 series sealant are true neutral curing silicone sealants that release methyl alcohol during cure while exposed to atmospheric moisture at room temperature. Unlike most alkoxy curing silicone sealants, RTV5240 series cures very rapidly. Key Performance Properties: A non-corrosive curing process that does not produce exothermic heat or corrosive by-products can be used on corrosion-sensitive electrical and electronic equipment with no adverse effectFast green strength build, fast cure (approximately 4x faster than traditional alkoxy sealants)Low odor cure by-productTough and resilient sealant with primerless adhesion to most metals, painted surfaces and plasticsUL recognized component, File number E-36952Superior hydrolytic stability. The RTV5240 series has demonstrated that it is able to maintain adhesion to many substrates after 20 weeks immersion in 60°C waterExcellent electrical insulation propertiesWithstands exposure to harsh environments such as chemical, ozone, moisture and weatheringCompatible with sensitive metals and plasticsGood tear resistanceEasy handling with no mixing, heating or solvent hazardsRetains elastomeric properties at temperatures of -75°F to 400°FApplications: The RTV5240 series are recommended for use in aerospace, automotive, appliance and other industries which incorporate electronic components or sensitive metal or plastic substrates into a finished product. Electronic and integrated circuits, semi conductors, and copper connections are typical applications. These products are also suitable for use in moist environments.The products in this series have fast green strength development and a cure time faster than many two-part sealants. Since they are one-part products, there is no mixing required, and they can be easily dispensed from a simple bulk dispensing pump or cartridges. Base/catalyst ratio control, static mixer maintenance, butterfly testing for mix uniformity, yield loss from base purging, and other activities/costs associated with two-part sealants are eliminated.GE Silicones became a part of Momentive Performance Materials in 2006.
Physical Properties Metric English Comments
Specific Gravity 1.50 g/cc
1.50 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 40
40
Tensile Strength, Ultimate 2.200 MPa
319.0 psi
Elongation at Break 425 %
425 %
Electrical Properties Metric English Comments
Volume Resistivity 3.00e+15 ohm-cm
3.00e+15 ohm-cm
Dielectric Constant 2.8

@Frequency 60 Hz
2.8

@Frequency 60 Hz
Dielectric Strength 20.0 kV/mm
508 kV/in
Dissipation Factor 0.0010

@Frequency 60 Hz
0.0010

@Frequency 60 Hz
Processing Properties Metric English Comments
Cure Time 45.0 min
0.750 hour
Tack-free
360 min
6.00 hour
To depth of 3.2 mm
Descriptive Properties Value Comments
Application rate 300 g/min
Color Gray
Sag/Slump 2.5 mm
Tooling time 10 min