Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | ASTM D257 |
Rogers Corporation TMM® TMM3 Ceramic Thermoset Polymer Composite TMM® Thermoset microwave materials are ceramic thermoset polymer composites designed for high plate-thru-hole reliability stripline and microstrip applications. The electrical and mechanical prope.. |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | 96 hours at 90°C; 50% RH; ASTM D257 |
PTS Tristar® PC-10FR-(VIK) 16 MFI Flame Retardant, UV Stabilized Polycarbonate With Impact Modifier and Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | after 96 hours at 90°C, 50% RH; ASTM D257 |
PTS Tristar® PC-10GFR 10% Glass Reinforced Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | after 96 hours at 90°C, 50% RH; ASTM D257 |
PTS Tristar® PC-10GFR-(V) 10% Glass Reinforced UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | |
Momentive Performance Materials RTV108 One Component Acetoxy Adhesive Sealant, Translucent RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. .. |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | |
Momentive Performance Materials RTV133 Black, Flame Retardant, One Component Silicone Sealant RTV 133 black, one-component, ready-to-use rubber adhesive sealant is recommended for evaluation in applications in the electronic, aerospace, appliance, transportation and other industries where re.. |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | |
Momentive Performance Materials RTV167 Electronic Grade Silicone Adhesive Sealant, Gray RTV160, RTV162, and RTV 167 adhesive sealants for GE silicones are one-component, ready-to-use electronic grade silicone sealants. They cure to a tough, resilient silicone rubber on exposure to atm.. |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | |
Momentive Performance Materials RTV5242 Neutral Cure, One Component RTV Adhesive Sealant RTV5240 series sealants are alkoxy neutral cure, one-component, ready to use, electronic grade silicone adhesive sealants exhibiting high strength that will maintain a strong bond even when exposed .. |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | |
Momentive Performance Materials RTV5243 Neutral Cure, One Component RTV Adhesive Sealant RTV5240 series sealants are alkoxy neutral cure, one-component, ready to use, electronic grade silicone adhesive sealants exhibiting high strength that will maintain a strong bond even when exposed .. |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | IEC 60093 |
Lanxess Durethan® DP 2131/20 W1 901317 Nylon 6, 20% Glass Fiber PA 6, injection molding grade, 20% glass fibers, better surface finish and resistance to alcoholic calcium chloride-solution than BKV 20 H2.0, weather resistance, good heat-ageing resistance |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6 GF33 HS L BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat Stabilizer Features: Lubricated and Heat StabilizedProcessi.. |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | ASTM D257 |
Techmer ES HiFill® PBT 1226 Availability: North AmericaForms: PelletsFeatures: Medium FlowAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | ASTM D257 |
Techmer ES HiFill® PBT 620 Availability: North AmericaForms: PelletsFeatures: Medium FlowAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | ASTM D257 |
Techmer ES HiFill® PBT WM35 X Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral FillerAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | ASTM D257 |
Techmer ES HiFill® PBT 0143 S Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | ASTM D257 |
Techmer ES HiFill® PBT 0150 S Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | ASTM D257 |
Techmer ES HiFill® PBT 0158 S Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | ASTM D257 |
Techmer ES HiFill® PBT GF/M40 BK 40% Glass/Mineral Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 40% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | IEC 60093 |
Polyplastics Duranex® 7407 Polybutylene Terephthalate (PBT), Super low warpage, GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | |
Loctite® 3534 Glob Top Encapsulant COB/DCA Encapsulants are essential to the reliability of flip chip assemblies because they minimize the thermal mismatch between the flip chip and substrate.Loctite® Underfills and Encapsulants imp.. |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | |
Dow Corning SE 738 SILICONE RTV One-part, white, moisture cure RTV, non-flowing, general purpose, UL 94 HB.Information provided by Dow Corning |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | IEC 60093 |
BASF Ultradur S 4090 G6 30% Glass Filled PBT Ultradur S 4090 G6 is a 30% glass reinforced PBT+ASA blend. It produces moldings with good surface finish, is resistant to chemicals and stress cracking, and has low shrinkage and warpage.Applicati.. |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | |
Aremco Aremco-Bond™ 2318 High Performance Epoxide |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | |
Resinlab® UR3010 Black Polyurethane Potting System Resinlab™ UR 3010 Black is a, two component, room temperature curing polyurethane potting system. It is designed to cure completely at room temperature. UR 3010 provides excellent environmental pro.. |
|||
Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | |
Resinlab® UR3010 Clear Polyurethane Potting System Resinlab™ UR 3010 Clear is a, two component, room temperature curing polyurethane potting system. It is designed to cure completely at room temperature. UR 3010 provides excellent environmental pro.. |