Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 2.200 MPa | 319.0 psi | |
Momentive Performance Materials RTV5242 Neutral Cure, One Component RTV Adhesive Sealant RTV5240 series sealants are alkoxy neutral cure, one-component, ready to use, electronic grade silicone adhesive sealants exhibiting high strength that will maintain a strong bond even when exposed .. |
|||
Tensile Strength, Ultimate | 2.200 MPa | 319.0 psi | |
Momentive Performance Materials RTV5243 Neutral Cure, One Component RTV Adhesive Sealant RTV5240 series sealants are alkoxy neutral cure, one-component, ready to use, electronic grade silicone adhesive sealants exhibiting high strength that will maintain a strong bond even when exposed .. |
|||
Tensile Strength, Ultimate | 2.200 MPa | 319.0 psi | |
Momentive Performance Materials RTV5249 Neutral Cure, One Component RTV Adhesive Sealant RTV5240 series sealants are alkoxy neutral cure, one-component, ready to use, electronic grade silicone adhesive sealants exhibiting high strength that will maintain a strong bond even when exposed .. |