Material Notes:
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances where quality is a key requirement. The Xantar® range includes: clear and tinted grades for transparent applicationsreinforced materialsFlame retardant and halogen free typeslubricated materials for added wear resistanceMitsubishi Engineering Plastics acquired the Xantar® product line from DSM in 2010.
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
ISO 1183
Viscosity Test 56 cm³/g
56 cm³/g
Limiting Viscosity Number; ISO 1628-4
Linear Mold Shrinkage, Flow 0.0020 cm/cm
0.0020 in/in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0040 cm/cm
0.0040 in/in
ISO 294-4
Melt Flow 5.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
5.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
Calculated from Volume Flow Rate of 4 cm<sup>3</sup>/10min.; ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell M 85
85
ISO 2039-2
Tensile Strength at Break 80.0 MPa
11600 psi
ISO 527-1/-2
Elongation at Break 5.0 %
5.0 %
ISO 527-1/-2
Tensile Modulus 3.50 GPa
508 ksi
ISO 527-1/-2
Flexural Strength 110 MPa
16000 psi
ISO 178
Flexural Modulus 3.70 GPa
537 ksi
ISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²

@Temperature 23.0 °C
4.76 ft-lb/in²

@Temperature 73.4 °F
ISO 180/4A
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 40.0 µm/m-°C

@Temperature 20.0 °C
22.2 µin/in-°F

@Temperature 68.0 °F
ISO 11359-1/-2
Maximum Service Temperature, Air 125 °C
257 °F
Ball Pressure Temperature; IEC 60695-10-2
Deflection Temperature at 1.8 MPa (264 psi) 143 °C
289 °F
ISO 75-1/-2
Vicat Softening Point 150 °C
302 °F
50°C/h 50N; ISO 306
UL RTI, Electrical 130 °C

@Thickness 1.50 mm
266 °F

@Thickness 0.0591 in
UL746B
130 °C

@Thickness 3.00 mm
266 °F

@Thickness 0.118 in
UL746B
UL RTI, Mechanical with Impact 125 °C

@Thickness 1.50 mm
257 °F

@Thickness 0.0591 in
UL746B
130 °C

@Thickness 3.00 mm
266 °F

@Thickness 0.118 in
UL746B
UL RTI, Mechanical without Impact 125 °C

@Thickness 1.50 mm
257 °F

@Thickness 0.0591 in
UL746B
130 °C

@Thickness 3.00 mm
266 °F

@Thickness 0.118 in
UL746B
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
IEC 60695-11-10
V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
IEC 60695-11-10
5VA

@Thickness 3.00 mm
5VA

@Thickness 0.118 in
IEC 60695-11-20
Oxygen Index 35 %
35 %
ISO 4589-1/-2
Glow Wire Test 825 °C

@Thickness 1.50 mm
1520 °F

@Thickness 0.0591 in
Glow Wire Ignition Temperature; IEC 60695-2-13
850 °C

@Thickness 3.00 mm
1560 °F

@Thickness 0.118 in
Glow Wire Ignition Temperature; IEC 60695-2-13
960 °C

@Thickness 3.00 mm
1760 °F

@Thickness 0.118 in
Glow Wire Flammability Index; IEC 60695-2-12
960 °C

@Thickness 1.50 mm
1760 °F

@Thickness 0.0591 in
Glow Wire Flammability Index; IEC 60695-2-12
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
IEC 60093
Surface Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
IEC 60093
Dielectric Constant 3.0

@Frequency 1e+6 Hz
3.0

@Frequency 1e+6 Hz
IEC 60250
3.1

@Frequency 100 Hz
3.1

@Frequency 100 Hz
IEC 60250
Dielectric Strength 29.0 kV/mm
737 kV/in
IEC 60243-1
Dissipation Factor 0.00090

@Frequency 100 Hz
0.00090

@Frequency 100 Hz
IEC 60250
0.0090

@Frequency 1e+6 Hz
0.0090

@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 200 V
200 V
IEC 60112
175 - 249 V
175 - 249 V
PLC 3; UL 746A
Descriptive Properties Value Comments
Flame Retardant Yes
Flame Retarding Agent Yes
Injection molding Yes
Release Agent Yes
With Fillers Yes