Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical without Impact | 125 °C @Thickness >=1.60 mm |
257 °F @Thickness >=0.0630 in |
|
LG Chemical LUCON SP9306FL sPS+MF Description Injection Molding Grade, sPS+MF, Low Thermal Conductivity, Chemical Resistance, High Heat ResistanceApplication: Electrical or Electronic Parts CAS No. 9003-53-6, 65997-17-3, 68928-70-1 .. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness >=3.00 mm |
257 °F @Thickness >=0.118 in |
|
LG Chemical Lupoy 1301EP-22 Polycarbonate Resin Description: LUPOY PC 1301EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness >=3.00 mm |
257 °F @Thickness >=0.118 in |
|
LG Chemical Lupoy 1301V-7 Polycarbonate Resin Description: LUPOY PC 1301V-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 0.750 mm |
257 °F @Thickness 0.0295 in |
UL746B |
Mitsubishi Xantar® 19 SR FD Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL746B |
Mitsubishi Xantar® 25 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL746B |
Mitsubishi Xantar® F 25 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL746B |
Mitsubishi Xantar® FC 19 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL746B |
Mitsubishi Xantar® FC 22 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL746B |
Mitsubishi Xantar® G2F 23 R Polycarbonate-10% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL746B |
Mitsubishi Xantar® G4F 22 UR Polycarbonate-20% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL746B |
Mitsubishi Xantar® G4F 23 UR Polycarbonate-20% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL746B |
Mitsubishi Xantar® G4F 25 R Polycarbonate-20% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL746B |
Mitsubishi Xantar® G4F 25 UR Polycarbonate-20% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL746B |
Mitsubishi Xantar® G6F 23 R Polycarbonate-30% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 1.60 - 1.70 mm |
257 °F @Thickness 0.0630 - 0.0669 in |
|
LG Chemical Lupoy 1200HP-15 Polycarbonate Resin Description: LUPOY PC 1200HP-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness >=3.00 mm |
257 °F @Thickness >=0.118 in |
|
LG Chemical LUPOY EF1006F PC, Halogen Free, Flame Retardant, High Heat Resistance Description: Injection Molding, PC, Halogen Free Flame Retardant, High Heat ResistanceApplication: IT/OA Housing and Components (Adaptor)CAS: 103598-77-2Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL746B |
DSM Stanyl® 46HF5040 Nylon 46-40% Glass Reinforced (European and Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL746B |
DSM Stanyl® TE250F8 Nylon 46-40% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 0.750 mm |
257 °F @Thickness 0.0295 in |
UL746B |
DSM Arnite® T06 200 (extrusion) PBT (European and Asian Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, DAM Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit.. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 3.00 mm |
257 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, DAM Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit.. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 0.750 mm |
257 °F @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® R525H BK02 Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525H BK02 is high-flow, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose.. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 3.00 mm |
257 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 41H Nylon 66, Impact Modified, DAM Vydyne® 41H is a general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne.. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL 746B |
Ascend Performance Materials Vydyne® 66J Nylon 66, General Purpose, high viscosity, DAM Vydyne® 66J is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66J resin offers high strength, .. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 22HSP Nylon 66, General Purpose, Heat Stabilized, DAM Availability:Asia PacificEuropeNorth America Additive:Lubricant Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood To.. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 0.750 mm |
257 °F @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® R530H Nylon 66, 30% Glass Filled, Dry as Molded Vydyne® R530H is a general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of phys.. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL746B |
Mitsubishi Xantar® 27 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances wher.. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, DAM Availability:Asia PacificEuropeNorth AmericaAdditive: Lubricant Features:Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood Tou.. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R533 Nylon 66, 33% Glass Filled, Dry as Molded Vydyne® R533 is general-purpose, 33% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for good machine feed, flow, and mold release. Glas.. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 3.00 mm |
257 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® R533 Nylon 66, 33% Glass Filled, Dry as Molded Vydyne® R533 is general-purpose, 33% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for good machine feed, flow, and mold release. Glas.. |